Polymer Property : Izod Impact, Unnotched = 8.81 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched 4.30 - 4.70 J/cm

@Temperature 23.0 °C
8.06 - 8.81 ft-lb/in

@Temperature 73.4 °F
ISO R180
Fainplast Compounds RH 4410 Rigid PVC, Antishock Extrusion
Antishock spiral pipes
Izod Impact, Unnotched 4.30 - 4.70 J/cm

@Temperature 23.0 °C
8.06 - 8.81 ft-lb/in

@Temperature 73.4 °F
ISO R180
Fainplast Compounds RL 455/AB Rigid PVC, Antishock Extrusion
Corrugated antishock electric pipes