Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 2.80 - 3.20 J/cm @Temperature 23.0 °C |
5.25 - 5.99 ft-lb/in @Temperature 73.4 °F |
ISO R180 |
Fainplast Compounds RH 206/C Rigid PVC, Antishock Extrusion Medium antishock profiles |
|||
Izod Impact, Unnotched | 2.80 - 3.20 J/cm @Temperature 23.0 °C |
5.25 - 5.99 ft-lb/in @Temperature 73.4 °F |
ISO R180 |
Fainplast Compounds RH 612 Rigid PVC, Antishock Extrusion Medium antishock profiles |
|||
Izod Impact, Unnotched | 2.80 - 3.20 J/cm @Temperature 23.0 °C |
5.25 - 5.99 ft-lb/in @Temperature 73.4 °F |
ISO R180 |
Fainplast Compounds RKS 311 Rigid PVC, Antishock Extrusion Lead Free Antishock profiles |
|||
Izod Impact, Unnotched | 1.60 - 3.20 J/cm | 3.00 - 5.99 ft-lb/in | Average value: 2.25 J/cm Grade Count:7 |
Overview of materials for Polyphenylene Sulfide (PPS), Stainless Steel Fiber This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), Stainless Steel Fiber". Each property range of values reported is minimum a.. |