Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 0.981 - 11.2 J/cm | 1.84 - 21.0 ft-lb/in | Average value: 7.34 J/cm Grade Count:21 |
Overview of materials for Polycarbonate, 30% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 30% Glass Filled". Specific grades with glass content between 25% and 34% are included. E.. |
|||
Izod Impact, Unnotched | 2.67 - 11.2 J/cm | 5.00 - 21.0 ft-lb/in | Average value: 5.02 J/cm Grade Count:38 |
Overview of materials for Polyetherimide (PEI), Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide, Carbon Fiber Filled". Each property range of values reported is minimum and maximum valu.. |
|||
Izod Impact, Unnotched | 2.14 - 11.2 J/cm | 4.00 - 21.0 ft-lb/in | Average value: 5.46 J/cm Grade Count:29 |
Overview of materials for Nylon 66, Aramid Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Aramid Fiber Filled". Each property range of values reported is minimum and maximum values of .. |
|||
Izod Impact, Unnotched | 3.74 - 11.2 J/cm | 7.00 - 21.0 ft-lb/in | Average value: 5.94 J/cm Grade Count:8 |
Overview of materials for Polyethersulfone (PES), 10% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone (PES), 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% a.. |
|||
Izod Impact, Unnotched | 5.87 - 11.2 J/cm | 11.0 - 21.0 ft-lb/in | Average value: 7.62 J/cm Grade Count:14 |
Overview of materials for Polyphthalamide (PPA), Glass Fiber 40% This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Glass Fiber 40%". Specific grades with glass content between 35% and 44% are included. .. |
|||
Izod Impact, Unnotched | 1.07 - 11.2 J/cm | 2.00 - 21.0 ft-lb/in | Average value: 3.74 J/cm Grade Count:17 |
Overview of materials for Polypropylene, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Carbon Fiber 10%". Each property range of values reported is minimum and maximum values o.. |