Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 4.96 J/cm @Temperature 23.0 °C |
9.29 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics LNP Faradex EX06464 PEI (Asia Pacific) LNP* Faradex* EX06464 is a compound based on Polyetherimide resin containing Stainless Steel. Added features of this material include: Electrically
Conductive, EMI/RFI Shielding.This data was suppli.. |
|||
Izod Impact, Unnotched | 4.96 J/cm | 9.29 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP ZP001XXP PPE+PS (Asia Pacific) LNP* Lubricomp* ZP001XXP is a compound based on PPE+PS Blend resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated. |
|||
Izod Impact, Unnotched | 4.96 J/cm | 9.29 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP RFB53XXZ PA 66 LNP* THERMOCOMP* RFB53XXZ is a compound based on Nylon 66 resin containing 15% Glass Fiber, 25% Glass Bead. |
|||
Izod Impact, Unnotched | 4.96 J/cm @Temperature -30.0 °C |
9.29 ft-lb/in @Temperature -22.0 °F |
ASTM D4812 |
SABIC Innovative Plastics NORYL GTX GTX8410W PPE+PA High flow, 10% Glass Reinforced PPE+PA. Typically used in Automotive connectors. |
|||
Izod Impact, Unnotched | 4.96 J/cm | 9.29 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP RF002 PA 66 LNP THERMOCOMP* RF002 is a compound based on Nylon 66 resin containing 10% Glass Fiber. |
|||
Izod Impact, Unnotched | 4.96 J/cm | 9.29 ft-lb/in | ASTM D256 |
A. Schulman ComAlloy Comtuf® 621 Nylon 6/6, Glass Reinforced, Impact Modified, Flow Enhanced Data provided by the manufacturer, ComAlloy International Company.13% Glass Reinforced. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been int.. |
|||
Izod Impact, Unnotched | 4.96 J/cm | 9.29 ft-lb/in | ASTM D256 |
A. Schulman ComAlloy Voloy® 431 Glass/Mineral Reinforced, PET Alloy, Flame Retardant, UL Data provided by the manufacturer, ComAlloy International Company.40% Glass/Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Izod Impact, Unnotched | 4.96 J/cm | 9.29 ft-lb/in | ASTM D256 |
A. Schulman ComAlloy Hiloy® 657 Nylon 6/6, Carbon/Glass Fiber Reinforced, Flow Enhanced Data provided by the manufacturer, ComAlloy International Company.The ComAlloy product line has been integrated into the A Schulman product line. |