Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 4.54 - 6.41 J/cm | 8.50 - 12.0 ft-lb/in | Average value: 5.52 J/cm Grade Count:10 |
Overview of materials for Polyetherimide (PEI), 20% Glass Fiber This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide, 20% Glass Fiber". Specific grades with glass content between 15% and 24% are included. E.. |
|||
Izod Impact, Unnotched | 4.54 J/cm | 8.50 ft-lb/in | ASTM D4812 |
A. Schulman SCHULAMID® 66 GF20H 20% Glass Fiber Reinforced, Heat Stabilized Nylon 66 Information provided by A. Schulman. |
|||
Izod Impact, Unnotched | 4.54 J/cm | 8.50 ft-lb/in | ASTM D4812 |
A. Schulman SCHULAMID® 66 GF20H 20% Glass Fiber Reinforced, Heat Stabilized Nylon 66 Information provided by A. Schulman. |
|||
Izod Impact, Unnotched | 4.54 J/cm | 8.50 ft-lb/in | ASTM D4812 |
A. Schulman SCHULAMID® 66 GF20H 20% Glass Fiber Reinforced, Heat Stabilized Nylon 66 Information provided by A. Schulman. |
|||
Izod Impact, Unnotched | 4.54 J/cm | 8.50 ft-lb/in | ASTM D4812 |
A. Schulman SCHULAMID® 66 GF20H 20% Glass Fiber Reinforced, Heat Stabilized Nylon 66 Information provided by A. Schulman. |