Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 4.50 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
8.43 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256 |
PolyOne Maxxam™ PPH-20C Nat Polypropylene Homopolymer (PP Homopolymer) PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car.. |
|||
Izod Impact, Unnotched | 4.50 J/cm | 8.43 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Primef® 4010 Polyphenylene Sulfide (PPS), 40% Glass Fiber Reinforcement
(discontinu Primef 4010 is a 40% glass fiber reinforced polyphenylene sulfide (PPS) that offers enhanced mechanical properties. In general, PPS offers an excellent balance of properties including high temperatu.. |
|||
Izod Impact, Unnotched | 4.50 J/cm | 8.43 ft-lb/in | ASTM D4812 |
Premix Premi-Glas® 2103-15 CRSX Polyester BMC Premi-Glas® 2103-15 CR-SX is a 15% glass reinforced thermoset Sheet Molding Compound designed for electrical switchgear and industrial circuit breaker applications. Key features and benefits are:U.. |
|||
Izod Impact, Unnotched | 4.50 - 4.50 J/cm @Temperature -40.0 - -40.0 °C |
8.43 - 8.43 ft-lb/in @Temperature -40.0 - -40.0 °F |
Average value: 4.07 J/cm Grade Count:1 |
Overview of materials for Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced". Each property range of values repor.. |
|||
Izod Impact, Unnotched | 4.50 - 4.50 J/cm @Thickness 3.20 - 3.20 mm |
8.43 - 8.43 ft-lb/in @Thickness 0.126 - 0.126 in |
Average value: 4.07 J/cm Grade Count:1 |
Overview of materials for Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced". Each property range of values repor.. |
|||
Izod Impact, Unnotched | 4.50 J/cm | 8.43 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Ixef® 1501/0003 Polyarylamide, 30% Glass Fiber, DAM
(discontinued **) The IXEF compounds are a family of semi-crystalline polyarylamide thermoplastics reinforced with glass fibers and/or mineral fillers for injection molding.Data provided by the manufacturer, Solvay A.. |
|||
Izod Impact, Unnotched | 4.50 J/cm - NB @Thickness 3.20 mm, Temperature 23.0 °C |
8.43 ft-lb/in - NB @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
Kingfa JH710 G10D Flame Retardant & 10% Glass Fiber Reinforced PC Features:Environmental friendly flame retardantUL V-0 @ 1.6mmHigh mechanical strengthGood size stability, good surfaceSuitable for exact moldingApplications:Exact mechanism partsElectrical and elect.. |
|||
Izod Impact, Unnotched | 4.50 J/cm - NB @Thickness 3.20 mm, Temperature 23.0 °C |
8.43 ft-lb/in - NB @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
Kingfa JH720 G10D 10% Glass Fiber Reinforced PC Features:Good processing propertiesLow tendency to warpHigh mechanical strengthGood size stabilityGood surfaceSuitable for exact moldingApplications:Exact mechanism partsPrinter, photocopies, scanne.. |
|||
Izod Impact, Unnotched | 4.50 J/cm @Thickness 3.20 mm, Temperature -40.0 °C |
8.43 ft-lb/in @Thickness 0.126 in, Temperature -40.0 °F |
ASTM D256 |
Kingfa LONOY 1300 PC/PBT Alloy Features:Excellent balance propertiesGood weather resistanceGood size stabilitySmooth surfaceUniform colorApplications:Injection moldingAutomobile bumperAutomobile interior/exterior trim partsBusine.. |
|||
Izod Impact, Unnotched | 4.50 J/cm | 8.43 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics ULTEM 2310EPR PEI 30% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing. |
|||
Izod Impact, Unnotched | 4.50 J/cm | 8.43 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics ULTEM 2310EPR PEI (Asia Pacific) 30% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing. |
|||
Izod Impact, Unnotched | 4.50 J/cm | 8.43 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics ULTEM 2310EPR PEI (Europe-Africa-Middle East) 30% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. Resin is RoHS compliant. UL94 V0 listing. |
|||
Izod Impact, Unnotched | 4.50 J/cm | 8.43 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP WL003 PBT LNP* LUBRICOMP* WL003 is a compound based on PBT resin containing 15% PTFE. Added feature of th is grade is: Wear Resistant. |
|||
Izod Impact, Unnotched | 4.50 J/cm | 8.43 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers AvaSpire® AV-722 SL30 Polyaryletherketone (PAEK) AV-722 SL30 is a wear resistant grade of AvaSpire® polyaryletherketone (PAEK) designed to provide low wear rates in both non-lubricated and lubricated environments. In addition to the outstanding.. |
|||
Izod Impact, Unnotched | 4.50 J/cm | 8.43 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Ixef® 3008 Polyarylamide (PARA), 30% Carbon Fiber Ixef® 3008 is a 30% carbon-fiber reinforced polyarylamide compound which exhibits extremely high strength and stiffness, good surface gloss, excellent creep resistance, and lower density than gla.. |
|||
Izod Impact, Unnotched | 4.50 J/cm @Thickness 3.18 mm |
8.43 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Solvay Specialty Polymers Ryton® R-4-230NA Polyphenylene Sulfide (PPS), 40% Glass Fiber Ryton® R-4-230NA and R-4-230BL 40% glass fiber reinforced polyphenylene sulfide compounds provide reduced flash and improved processability compared to other polyphenylene sulfide injection moldi.. |
|||
Izod Impact, Unnotched | 4.50 J/cm @Thickness 3.18 mm |
8.43 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Solvay Specialty Polymers Ryton® R-4-232NA Polyphenylene Sulfide (PPS), 40% Glass Fiber Ryton® R-4-232NA 40% glass fiber reinforced polyphenylene sulfide compound complies with United States Food and Drug Administration (FDA) and European Union (EU 10/2011 and 1183/2012) regulations.. |
|||
Izod Impact, Unnotched | 4.50 J/cm | 8.43 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Valox® ENH8560 PBT+PET (Europe-Africa-Middle East) Non-Brominated & Non-Chlorinated Flame Retardant, 30% Glass fiber reinforced PBT/PET blend |
|||
Izod Impact, Unnotched | 4.50 J/cm | 8.43 ft-lb/in | ASTM D256 |
Adell ER-19 Polypropylene Homopolymer; 43% Glass Reinforced, High Stiffness Data provided by Adell Plastics, Inc. |
|||
Izod Impact, Unnotched | 4.50 J/cm | 8.43 ft-lb/in | ASTM D256 |
Adell ER-39 Polypropylene Homopolymer; 43% Glass Reinforced, High Stiffness Data provided by Adell Plastics, Inc. |
|||
Izod Impact, Unnotched | 4.50 J/cm | 8.43 ft-lb/in | ISO 180 |
Solvay Specialty Polymers Ixef® 3006/9019 Polyarylamide, 30% Carbon Fiber, DAM
(discontinued **) The IXEF compounds are a family of semi-crystalline polyarylamide thermoplastics reinforced with glass fibers and/or mineral fillers for injection molding.Data provided by the manufacturer, Solvay A.. |