Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 4.06 J/cm | 7.60 ft-lb/in | ASTM D4812 |
A. Schulman VOLOY™ 414 30% Glass Fiber Reinforced, Flame Retardant PBT Information provided by A. Schulman. |
|||
Izod Impact, Unnotched | 4.06 J/cm | 7.60 ft-lb/in | ASTM D4812 |
A. Schulman ComAlloy® E-12812 Easy Flow Glass Reinforced Nylon 66 Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Izod Impact, Unnotched | 4.06 J/cm | 7.60 ft-lb/in | ASTM D4812 |
A. Schulman ComAlloy® E-12812 Easy Flow Glass Reinforced Nylon 66 Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Izod Impact, Unnotched | 4.06 J/cm | 7.60 ft-lb/in | ASTM D4812 |
A. Schulman VOLOY™ 414 30% Glass Fiber Reinforced, Flame Retardant PBT Information provided by A. Schulman. |
|||
Izod Impact, Unnotched | 4.06 J/cm | 7.60 ft-lb/in | ASTM D4812 |
A. Schulman VOLOY™ 414 30% Glass Fiber Reinforced, Flame Retardant PBT Information provided by A. Schulman. |
|||
Izod Impact, Unnotched | 4.06 J/cm | 7.60 ft-lb/in | ASTM D4812 |
A. Schulman ComAlloy® E-12812 Easy Flow Glass Reinforced Nylon 66 Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Izod Impact, Unnotched | 4.06 J/cm | 7.60 ft-lb/in | ASTM D4812 |
A. Schulman ComAlloy® E-12812 Easy Flow Glass Reinforced Nylon 66 Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Izod Impact, Unnotched | 4.06 J/cm | 7.60 ft-lb/in | ASTM D4812 |
A. Schulman VOLOY™ 414 30% Glass Fiber Reinforced, Flame Retardant PBT Information provided by A. Schulman. |
|||
Izod Impact, Unnotched | 4.06 J/cm | 7.60 ft-lb/in | ASTM D4812 |
A. Schulman ComAlloy® E-12812 Easy Flow Glass Reinforced Nylon 66 Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Izod Impact, Unnotched | 4.06 J/cm | 7.60 ft-lb/in | ASTM D4812 |
A. Schulman VOLOY™ 414 30% Glass Fiber Reinforced, Flame Retardant PBT Information provided by A. Schulman. |
|||
Izod Impact, Unnotched | 4.06 J/cm | 7.60 ft-lb/in | ASTM D4812 |
A. Schulman ComAlloy® E-12812 Easy Flow Glass Reinforced Nylon 66 Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Izod Impact, Unnotched | 4.06 J/cm | 7.60 ft-lb/in | ASTM D4812 |
A. Schulman VOLOY™ 414 30% Glass Fiber Reinforced, Flame Retardant PBT Information provided by A. Schulman. |