Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 4.00 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
7.49 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256 |
PolyOne Maxxam™ PD 2201 Polypropylene, Unspecified (PP, Unspecified) PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car.. |
|||
Izod Impact, Unnotched | 4.00 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
7.49 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256 |
PolyOne Maxxam™ PPH-40C Nat Polypropylene Homopolymer (PP Homopolymer) PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car.. |
|||
Izod Impact, Unnotched | 4.00 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
7.49 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256 |
PolyOne Trilliant™ HC X HC5200-0026 RS Natural Polypropylene, Unspecified (PP, Unspecified) Information provided by PolyOne |
|||
Izod Impact, Unnotched | 4.00 J/cm @Thickness 4.00 mm, Temperature 23.0 °C |
7.49 ft-lb/in @Thickness 0.157 in, Temperature 73.4 °F |
ISO 180 |
Premix Thermoplastics PRE-ELEC® ESD 7120 PRE-ELEC ESD 7120 is a static dissipative thermoplastic compound based on ABS. The dissipative property is permanent and built into the polymer chain. PRE-ELEC ESD 7120 has been developed for inject.. |
|||
Izod Impact, Unnotched | 4.00 J/cm | 7.49 ft-lb/in | ISO 180 |
Solvay Specialty Polymers Primef® 5084 30% GF PPS, Lubricated Grade
(discontinued **) Contains PTFE lubricant. Used for injection molding of high performance parts. |
|||
Izod Impact, Unnotched | 4.00 J/cm @Thickness 3.18 mm |
7.49 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
LNP Stat-Kon® LC-1003 EM Polyetheretherketone, Carbon Fiber Reinforcement
(discontinued **) Features: Good Moldability, Electrically ConductiveForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; howev.. |
|||
Izod Impact, Unnotched | 4.00 J/cm @Thickness 3.18 mm |
7.49 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Solvay Specialty Polymers Ryton® R-4 Polyphenylene Sulfide (PPS), 40% Glass Fiber Ryton® R-4 and R-4-02 40% glass fiber reinforced polyphenylene sulfide compounds provide a good combination of mechanical and electrical properties with outstanding chemical resistance, even at e.. |
|||
Izod Impact, Unnotched | 4.00 J/cm @Thickness 3.18 mm |
7.49 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Solvay Specialty Polymers Ryton® R-4-230BL Polyphenylene Sulfide (PPS), 40% Glass Fiber Ryton® R-4-230NA and R-4-230BL 40% glass fiber reinforced polyphenylene sulfide compounds provide reduced flash and improved processability compared to other polyphenylene sulfide injection moldi.. |
|||
Izod Impact, Unnotched | 4.00 J/cm | 7.49 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Valox® 855 PBT (Europe-Africa-Middle East) VALOX 855 is 15% glass reinforced PBT+PET blend with improved surface appearance. Applications: external housings, steam irons, appliance housings and lighting parts. |
|||
Izod Impact, Unnotched | 4.00 J/cm @Temperature -30.0 °C |
7.49 ft-lb/in @Temperature -22.0 °F |
ASTM D4812 |
SABIC Innovative Plastics Valox® 855 PBT (Europe-Africa-Middle East) VALOX 855 is 15% glass reinforced PBT+PET blend with improved surface appearance. Applications: external housings, steam irons, appliance housings and lighting parts. |
|||
Izod Impact, Unnotched | 4.00 J/cm | 7.49 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Valox® ENH4530 PBT (Europe-Africa-Middle East) 15% GF PBT, Non-Brominated & Non-Chlorinated Flame retardant |
|||
Izod Impact, Unnotched | 4.00 J/cm @Temperature -30.0 °C |
7.49 ft-lb/in @Temperature -22.0 °F |
ASTM D4812 |
SABIC Innovative Plastics Valox® ENH8560 PBT+PET (Europe-Africa-Middle East) Non-Brominated & Non-Chlorinated Flame Retardant, 30% Glass fiber reinforced PBT/PET blend |
|||
Izod Impact, Unnotched | 4.00 J/cm @Temperature 23.0 °C |
7.49 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics LNP Stat-kon EE008E PEI LNP STAT-KON* EE008E is a compound based on Polyetherimide resin containing Carbon Fiber. Added features of this material include: Easy Molding.This data was supplied by SABIC-IP for the Americas r.. |
|||
Izod Impact, Unnotched | 4.00 J/cm | 7.49 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Valox® K4530 PBT (Europe-Africa-Middle East) 15% glass reinforced PBT, Hydrolytically stable, High flow, Automotive connectors. |
|||
Izod Impact, Unnotched | 4.00 J/cm | 7.49 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP LC003E PEEK LNP THERMOCOMP* LC003E is a compound based on Polyetheretherketone resin containing 15% Carbon Fiber. Added features of this material include: Easy Molding, Electrically Conductive |
|||
Izod Impact, Unnotched | 4.00 J/cm | 7.49 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP LC003E PEEK (Asia Pacific) LNP THERMOCOMP* LC003E is a compound based on Polyetheretherketone resin containing Carbon Fiber. Added features of this material include: Easy Molding. |
|||
Izod Impact, Unnotched | 4.00 J/cm @Temperature 23.0 °C |
7.49 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics LNP Thermocomp RW008XXZ PA 66 LNP* Thermocomp* RW008XXZ is a compound based on Nylon 6/6 resin containing Wollastonite.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Unnotched | 4.00 J/cm | 7.49 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP DB008ERP PC LNP* THERMOCOMP* DB008ERP is a compound based on Polycarbonate resin containing 40% Glass Bead. Added features of this material include: Easy Molding, Mold Release. |
|||
Izod Impact, Unnotched | 4.00 J/cm | 7.49 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP DB008ERP PC (Asia Pacific) LNP* Thermocomp* DB008ERP is a compound based on Polycarbonate resin containing Glass Bead. Added features of this material include: Easy Molding, Mold Release. |
|||
Izod Impact, Unnotched | 4.00 J/cm | 7.49 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics NORYL FE1520PW PPE+PS (Europe-Africa-Middle East) Noryl* FE1520PW resin is a blend of polyphenylene oxide (PPO) and polystyrene (PS) resin that contains 20% glass reinforcement. The resin is suitable for injection molding. Noryl FE1520PW resin has .. |
|||
Izod Impact, Unnotched | 4.00 J/cm | 7.49 ft-lb/in | ASTM D256 |
A. Schulman ComAlloy Aqualoy® 135 Polypropylene, Glass Reinforced, Chemically Coupled NSF, UL Data provided by the manufacturer, ComAlloy International Company.35% Glass Reinforced. In Aqualoy® materials, carefully selected base resins and proprietary additives meld hydrolytic stability an.. |
|||
Izod Impact, Unnotched | 4.00 J/cm | 7.49 ft-lb/in | ASTM D256 |
A. Schulman ComAlloy E-16674B PPS, Electrically Conductive - Carbon Fiber Filled Data provided by the manufacturer, ComAlloy International Company.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Izod Impact, Unnotched | 4.00 J/cm | 7.49 ft-lb/in | ASTM D256 |
A. Schulman ComAlloy Voloy® 413 Polyester - PBT, Glass Reinforced, Flame Retardant, UL Data provided by the manufacturer, ComAlloy International Company.30% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Izod Impact, Unnotched | 4.00 J/cm | 7.49 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP Lexan_LGN2000A PC (Europe-Africa-Middle East) LNP* Thermocomp* Lexan_LGN2000A compound is a 20% glass reinforced PC, high flow. UL rated V-0. Consumer Electronics applications. |
|||
Izod Impact, Unnotched | 4.00 J/cm | 7.49 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Valox® K4530 PBT 15% glass reinforced PBT, Hydrolytically stable, High flow, Automotive connectors. |
|||
Izod Impact, Unnotched | 4.00 J/cm | 7.49 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Valox® VX4510 PBT (Europe-Africa-Middle East) VALOX VX4510 is a flame retarded, 10% glassfiber reinforced injection moulding PBT resin. |