Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 32.04 J/cm | 60.02 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Lexan® 103 PC UL rated HB as of 10/97. 200 series recommended when V-2 rating required. Nonhalogenated. 7.0 MFR, for thicker sections without sinks. UV stabilized for outdoor and lighting. |
|||
Izod Impact, Unnotched | 32.04 J/cm | 60.02 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Lexan® 104R PC UL rated HB. 200 series recommended when V-2 rating required. 7.0 MFR, for thicker sections without sinks. Internal mold release. FDA food contact compliant in limited colors.Effective January 15.. |
|||
Izod Impact, Unnotched | 32.04 J/cm | 60.02 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Lexan® 131 PC Nonhalogenated. 3.5 MFR. |
|||
Izod Impact, Unnotched | 32.04 J/cm | 60.02 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Lexan® 131R PC (Asia Pacific) Nonhalogenated. 3.5 MFR. |
|||
Izod Impact, Unnotched | 32.04 J/cm | 60.02 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Lexan® 191 PC (Asia Pacific) Nonhalogenated. 8.5 MFR. High impact. Thick wall sections. Opaques only. |
|||
Izod Impact, Unnotched | 32.04 J/cm | 60.02 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Lexan® 223R PC 17.5 MFR, for small, intricate parts. Improved flame retardance. Internal mold release. UV stabilized. |
|||
Izod Impact, Unnotched | 32.04 J/cm | 60.02 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Lexan® 4504 PPC High heat resistant polycarbonate copolymer, provides DTUL of 290F at 264 psi. FDA food contact compliant in limited colors. Effective January 15th, 2008 this grade will no longer be supported with .. |
|||
Izod Impact, Unnotched | 32.04 J/cm | 60.02 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Lexan® 4704 PPC High heat resistant polycarbonate copolymer, provides DTUL of 300F at 264 psi. FDA food contact compliant in limited colors. Effective January 15th, 2008 this grade will no longer be supported with .. |
|||
Izod Impact, Unnotched | 32.04 J/cm | 60.02 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Lexan® 923A PC (Asia Pacific) Low viscosity, flame retardant with exceptional surface. Clear, tints and opaque colors. UV-stabilized. |
|||
Izod Impact, Unnotched | 32.04 J/cm | 60.02 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Lexan® 943A PC Medium viscosity, superior flame retardance. UV-Stabilized. Clear, tints and opaque colors. |
|||
Izod Impact, Unnotched | 32.04 J/cm | 60.02 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Lexan® EXL6414 PC PC-Siloxane copolymer with excellent processability. Impact modified, medium flow, extreme low temp. ductility. |
|||
Izod Impact, Unnotched | 32.04 J/cm @Temperature 23.0 °C |
60.02 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics Lexan® FXD103 PC FXD103 is a Light Diffusion effect, part of the VisualFX family. These effects have been developed to meet increasing Aesthetic demands in the Marketplace.This data was supplied by SABIC-IP for the .. |
|||
Izod Impact, Unnotched | 32.04 J/cm | 60.02 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Lexan® HP1R PC (Asia Pacific) High flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO sterilizable. Contains a higher amount.. |
|||
Izod Impact, Unnotched | 32.04 J/cm | 60.02 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Lexan® HPS6 PC (Asia Pacific) Med/low flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam e-beam and gamma sterilizable. .. |
|||
Izod Impact, Unnotched | 32.04 J/cm | 60.02 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Lexan® LI1911R PC Low-viscosity multi-purpose PC having low levels of ionics species. Internal mold release. |
|||
Izod Impact, Unnotched | 32.04 J/cm @Temperature 23.0 °C |
60.02 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics Lexan® PPC4504 PPC High heat resistant polycarbonate copolymer, provides DTUL of 290F at 264 psi. FDA food contact compliant in limited colors. Effective January 15th, 2008 this grade will no longer be supported wit.. |
|||
Izod Impact, Unnotched | 32.04 J/cm @Temperature 23.0 °C |
60.02 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics Lexan® 151 PC Nonhalogenated. 2.5 MFR. Blowmolding/extrusion.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Unnotched | 32.04 J/cm | 60.02 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Lexan® 243R PC (Asia Pacific) 10.5 MFR. UV-stabilized. Improved flame retardance. Internal mold release. |
|||
Izod Impact, Unnotched | 32.04 J/cm | 60.02 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Lexan® 940A PC Medium viscosity, flame retardant PC. Exceptional surface. Clear, tints and opaque colors. |
|||
Izod Impact, Unnotched | 32.04 J/cm | 60.02 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Lexan® 950A PC (Asia Pacific) Transparent, clear and colors, high viscosity, flame retardant with exceptional surface. |
|||
Izod Impact, Unnotched | 32.04 J/cm @Temperature 23.0 °C |
60.02 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics Lexan® FXE101R PC Transparent PC. ILLUMINATE special effects (fluorescent/edge glow colors). For thicker sections without sinks. Internal mold release.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Unnotched | 32.04 J/cm | 60.02 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Lexan® HP6NR PC (Asia Pacific) Low/med flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains no .. |
|||
Izod Impact, Unnotched | 32.04 J/cm | 60.02 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Lexan® HPS6R PC Low/med flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). Contains a higher amount of mold release t.. |
|||
Izod Impact, Unnotched | 32.04 J/cm | 60.02 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics NORYL GTX GTX902 PPE+PS+PA (Asia Pacific) Unreinforced. Excellent chemical resistance and paintability. 312F (155C) HDT. |
|||
Izod Impact, Unnotched | 32.04 J/cm | 60.02 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Lexan® 103R PC UL rated HB as of 10/97. 200 series recommended when V-2 rating required. Nonhalogenated. 7.0 MFR, for thicker sections without sinks. UV Stabilized for outdoor and lighting. Internal mold release... |
|||
Izod Impact, Unnotched | 32.04 J/cm @Temperature 23.0 °C |
60.02 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics Lexan® SFX123RU PC (Asia Pacific) SFX123RU is a transparent SecurFX grade with improved flow, mold release and UV stabilizer. This grade is for security applications and contains proprietary authentication technology.This data was s.. |
|||
Izod Impact, Unnotched | 32.04 J/cm | 60.02 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Lexan® 143R PC (Asia Pacific) Nonhalogenated. 10.5 MFR. UV-stabilized. Internal mold release. |
|||
Izod Impact, Unnotched | 32.04 J/cm | 60.02 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Lexan® 950 PC (Asia Pacific) Opaque colors, high viscosity, superior flame retardance. |
|||
Izod Impact, Unnotched | 32.04 J/cm | 60.02 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Lexan® HP4NR PC (Asia Pacific) Medium flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains no m.. |
|||
Izod Impact, Unnotched | 32.04 J/cm | 60.02 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Lexan® HP4NR PC (Europe-Africa-Middle East) Medium flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains no m.. |