Polymer Property : Izod Impact, Unnotched = 6.99 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched 3.73 J/cm
6.99 ft-lb/in
ASTM D4812
SABIC Innovative Plastics Valox® 771 PBT
35% mineral/glass reinforced flame retardant grade with a CTI performance level class of 0 rating. Applications which may see electrical arcing.
Izod Impact, Unnotched 3.73 J/cm
6.99 ft-lb/in
ASTM D4812
SABIC Innovative Plastics Valox® 780 PBT
40% gl/min, UL94 V-0 rated. Nonblooming flame retardant. Circuit breaker handles/housings, motor coil housings.
Izod Impact, Unnotched 3.73 J/cm
6.99 ft-lb/in
ASTM D4812
SABIC Innovative Plastics Valox® 780 PBT (Asia Pacific)
40% gl/min, UL94 V-0 rated. Nonblooming flame retardant. Circuit breaker handles/housings, motor coil housings.
Izod Impact, Unnotched 3.73 J/cm
6.99 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP STAT-KON DX05474 PC
LNP* STAT-KON* DX05474 is a compound based on Polycarbonate resin containing 10% Carbon Fiber. Added features of this material include: Electrically Conductive, Easy Molding, Flame Retardant, Mold ..
Izod Impact, Unnotched 3.73 J/cm
6.99 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP STAT-KON DX05474 PC (Asia Pacific)
LNP* Stat-kon* DX05474 is a compound based on Polycarbonate resin containing Flame Retardant, Carbon Fiber. Added features of this material include: Electrically Conductive, Easy Molding, Flame Ret..
Izod Impact, Unnotched 3.73 J/cm
6.99 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP STAT-KON EE003XXC PEI
LNP STAT-KON* EE003XXC is a compound based on Polyetherimide resin containing 15% Carbon Fiber. Added features of this material include: Clean Compound System, Electrically Conductive.
Izod Impact, Unnotched 3.73 J/cm
6.99 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP STAT-KON EE003XXC PEI (Asia Pacific)
LNP* STAT-KON* EE003XXC is a compound based on Polyetherimide resin containing Carbon Fiber. Added features of this material include: Clean Compounding System.
Izod Impact, Unnotched 3.73 J/cm
6.99 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP STAT-KON KX02764 Acetal
LNP STAT-KON* KX02764 is a compound based on Acetal resin containing Proprietary Filler(s). Added feature of this material is: Electrically Conductive.
Izod Impact, Unnotched 3.73 J/cm

@Temperature 23.0 °C
6.99 ft-lb/in

@Temperature 73.4 °F
ASTM D 4812
SABIC Innovative Plastics LNP Stat-kon WFD059 PBT (Asia Pacific)
LNP* Stat-kon* WFD059 is a compound based on Polybutylene Terephalate resin containing Glass Fiber, Flame Retardant. Added features of this material include: Flame Retardant.This data was supplied ..
Izod Impact, Unnotched 3.73 J/cm
6.99 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP THERMOCOMP DX06413H PC
LNP* THERMOCOMP* DX06413H is a compound based on Polycarbonate resin containing 40% Glass Fiber. Added features of this material include: Easy Molding, Mold Release.
Izod Impact, Unnotched 3.73 J/cm
6.99 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP THERMOCOMP EC006 PEI
LNP THERMOCOMP* EC006 is a compound based on Polyetherimide resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive.
Izod Impact, Unnotched 3.73 J/cm
6.99 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP THERMOCOMP EC006 PEI (Asia Pacific)
LNP THERMOCOMP* EC006 is a compound based on Polyetherimide resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.
Izod Impact, Unnotched 3.73 J/cm

@Temperature 23.0 °C
6.99 ft-lb/in

@Temperature 73.4 °F
ASTM D 4812
SABIC Innovative Plastics Ultem 2110N PEI (Asia Pacific)
10% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming.This data was supplied by SABIC-IP for the Asia Pacific region.
Izod Impact, Unnotched 3.73 J/cm
6.99 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP STAT-KON DEL329E PC
LNP* Stat-kon* DEL329E is a compound based on Polycarbonate resin containing 10% Carbon Fiber, 15% PTFE. Added features of this material include: Electrically Conductive, Flame Retardant, Wear Resi..
Izod Impact, Unnotched 3.73 J/cm
6.99 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP STAT-KON DX03633C PC
LNP STAT-KON* DX03633C is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added features of this material include: Clean Compounding System, Electrically Conductive.
Izod Impact, Unnotched 3.73 J/cm

@Temperature 23.0 °C
6.99 ft-lb/in

@Temperature 73.4 °F
ASTM D 4812
SABIC Innovative Plastics LNP Stat-kon WFD059 PBT
LNP* Stat-kon* WFD059 is a compound based on Polybutylene Terephalate resin containing Glass Fiber, Flame Retardant. Added features of this material include: Flame Retardant.This data was supplied ..
Izod Impact, Unnotched 3.73 J/cm
6.99 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP THERMOCOMP AF004L ABS (Asia Pacific)
LNP* Thermocomp* AF004L is a compound based on Acrylonitrile Butadiene Styrene resin containing Glass Fiber. Added features of this material include: Low Extractible.
Izod Impact, Unnotched 3.73 J/cm

@Temperature 23.0 °C
6.99 ft-lb/in

@Temperature 73.4 °F
ASTM D 4812
SABIC Innovative Plastics Ultem 2110N PEI
10% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming.This data was supplied by SABIC-IP for the Americas region.