Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 3.68 J/cm | 6.90 ft-lb/in | ASTM D256 |
Styron EMERGEâ„¢ 4702-15 Polycarbonate EMERGEâ„¢ PC 4702-15 advanced resin is formulated with 20% glass fiber and a proprietary flame retardant package. It provides good ignition resistance, rigidity, dimension stability and heat res.. |
|||
Izod Impact, Unnotched | 3.68 J/cm | 6.90 ft-lb/in | ASTM D4812 |
A. Schulman ComAlloy® E-13819 Heat Dissipative PPS Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Izod Impact, Unnotched | 3.68 J/cm | 6.90 ft-lb/in | ASTM D4812 |
A. Schulman ComAlloy® E-13819 Heat Dissipative PPS Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Izod Impact, Unnotched | 3.68 J/cm | 6.90 ft-lb/in | ASTM D4812 |
A. Schulman ComAlloy® E-13819 Heat Dissipative PPS Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Izod Impact, Unnotched | 3.68 J/cm | 6.90 ft-lb/in | ASTM D4812 |
A. Schulman ComAlloy® E-13819 Heat Dissipative PPS Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Izod Impact, Unnotched | 3.68 J/cm | 6.90 ft-lb/in | ASTM D4812 |
A. Schulman ComAlloy® E-13819 Heat Dissipative PPS Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Izod Impact, Unnotched | 3.68 J/cm | 6.90 ft-lb/in | ASTM D4812 |
A. Schulman ComAlloy® E-13819 Heat Dissipative PPS Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |