Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 3.36 J/cm | 6.29 ft-lb/in | ASTM D256 |
Proto3000 Duraform® PA Selective Laser Sintering (SLS®) Prototyping Polymer Description: Durable polyamide (nylon) material for real-world physical testing and functional useFeatures: Excellent surface resolution and feature detailEasy-to-processCompliant with USP Class VI .. |
|||
Izod Impact, Unnotched | 3.36 J/cm | 6.29 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP DX00714H PC LNP LUBRICOMP* DX00714H is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added features of this material include: Wear Resistant, Healthcare. |
|||
Izod Impact, Unnotched | 3.36 J/cm | 6.29 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP DX00714H PC (Asia Pacific) LNP LUBRICOMP* DX00714H is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added features of this material include: Internally Lubricated. |
|||
Izod Impact, Unnotched | 3.36 J/cm @Temperature 23.0 °C |
6.29 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics LNP Thermocomp FF004 PE (Asia Pacific) LNP* THERMOCOMP* FF004 is a compound based on Polyethylene resin containing Glass Fiber.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Unnotched | 3.36 J/cm | 6.29 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP SH0700B PA12 LNP* Thermocomp* SH0700B is a compound based on Nylon 12 containing proprietary fillers. Added feature: High Specific Gravity |
|||
Izod Impact, Unnotched | 3.36 J/cm | 6.29 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOTUF MX00619 PP LNP* Thermotuf* MX00619 is a compound based on Polypropylene resin containing Proprietary Filler(s). |
|||
Izod Impact, Unnotched | 3.36 J/cm @Temperature 23.0 °C |
6.29 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
3D Systems DuraForm® PA Nylon for SLS® Systems For use with all selective laser sintering (SLS®) systems.ApplicationsComplex, thin-wall ductworkMotorsportsAerospaceHousings and enclosuresImpellers and connectorsConsumer sporting goodsVehicle da.. |
|||
Izod Impact, Unnotched | 3.36 J/cm | 6.29 ft-lb/in | ASTM D256 |
A. Schulman ComAlloy Voloy® 682 Nylon 6/6, Glass Fiber, Nylon 6/6 Alloy, Flame Retardant, UL Data provided by the manufacturer, ComAlloy International Company.45% Glass Reinforced. Halogen- and phosphorous-freeThe ComAlloy product line has been integrated into the A Schulman product line. |
|||
Izod Impact, Unnotched | 3.36 J/cm | 6.29 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOTUF MX00619 PP (Asia Pacific) LNP* Thermotuf* MX00619 is a compound based on Polypropylene resin containing Proprietary Filler(s). |
|||
Izod Impact, Unnotched | 3.36 - 5.34 J/cm | 6.29 - 10.0 ft-lb/in | Average value: 4.04 J/cm Grade Count:5 |
Overview of materials for Polystyrene + Polyphenylene Ether, Glass Filler This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene + Polyphenylene Ether, Glass Filler". Each property range of values reported is minimum and .. |