Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 3.20 - 5340 J/cm | 6.00 - 10000 ft-lb/in | Average value: 8.92 J/cm Grade Count:19 |
Overview of materials for Polypropylene with 40% Calcium Carbonate (CaCO3) Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Calcium Carbonate (CaCO3) Filler". Specific grades with primary filler content be.. |
|||
Izod Impact, Unnotched | 3.20 - 60.0 J/cm | 6.00 - 112 ft-lb/in | Average value: 8.89 J/cm Grade Count:34 |
Overview of materials for Nylon 66, 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 20% Glass Fiber Filled". Specific grades with glass content between 15% and 24% are included. .. |
|||
Izod Impact, Unnotched | 3.20 - 5.34 J/cm | 6.00 - 10.0 ft-lb/in | Average value: 3.74 J/cm Grade Count:9 |
Overview of materials for Nylon 66, Mineral Filled, NCG Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Mineral Filled, NCG Fiber Filled". Each property range of values reported is minimum and maxim.. |
|||
Izod Impact, Unnotched | 3.20 J/cm | 6.00 ft-lb/in | ASTM-D256 |
Ineos ABS Lustran® SAN DN77 SAN Grade Lustran® SAN DN77 is a natural color, styrene-acrylonitrile copolymer supplied in pellet form. It is designed for use in compounding. |
|||
Izod Impact, Unnotched | 3.20 J/cm @Thickness 3.17 mm |
6.00 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® ABS GF5 5% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 5% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Izod Impact, Unnotched | 3.20 J/cm @Thickness 3.17 mm |
6.00 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® ABS GF50 50% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Izod Impact, Unnotched | 3.20 J/cm @Thickness 3.17 mm |
6.00 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® HDPE TM10 10% Talc Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Talc Filler, 10% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Izod Impact, Unnotched | 3.20 J/cm @Thickness 3.17 mm |
6.00 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® PA6/6 CM40 40% Mineral Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Mineral Filler, 40% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Heat Stabilized and LubricatedAppearance: Natural .. |
|||
Izod Impact, Unnotched | 3.20 J/cm @Thickness 3.17 mm |
6.00 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES Luriblend® PC CF15 TL6 BK 15% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 10% Filler by WeightAdditive: PTFE LubricantFeatures: LubricatedAppearance: BlackInformation provided by TP Composites, I.. |
|||
Izod Impact, Unnotched | 3.20 J/cm @Thickness 3.17 mm |
6.00 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® ABS GF20 FR 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Izod Impact, Unnotched | 3.20 J/cm | 6.00 ft-lb/in | ASTM D4812 |
Asahi Kasei Thermofil N5-15FG-1103 15% Glass Fiber Reinforced, Lubricated Information provided by Asahi Thermofil |
|||
Izod Impact, Unnotched | 3.20 - 6.41 J/cm | 6.00 - 12.0 ft-lb/in | Average value: 4.34 J/cm Grade Count:4 |
Overview of materials for Polyphenylene Ether, 30% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, 30% Glass Filled". Specific grades with glass content between 25% and 34% are inclu.. |