Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 2.90 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
5.43 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256 |
PolyOne Gravi-Tech™ GRV-NY-085-W-NAT Polyamide 6 (Nylon 6) Information provided by PolyOne |
|||
Izod Impact, Unnotched | 2.90 J/cm | 5.43 ft-lb/in | ASTM D256 |
Chevron Phillips Ryton® R-7 Polyphenylene Sulfide Compound
(discontinued **) Natural Color Polyphenylene Sulfide CompoundRyton® R-7 is polyphenylene sulfide compounded with glass fibers and mineral fibers to produce an injection moldable high temperature engineering compoun.. |
|||
Izod Impact, Unnotched | 2.90 J/cm | 5.43 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Ixef® 2530/X9027 Polyarylamide, 55% Mineral + Glass Fiber, DAM
(discontinued **)< The IXEF compounds are a family of semi-crystalline polyarylamide thermoplastics reinforced with glass fibers and/or mineral fillers for injection molding.Data provided by the manufacturer, Solvay A.. |
|||
Izod Impact, Unnotched | 2.90 J/cm | 5.43 ft-lb/in | ASTM D256 |
Adell RA-18 Copolymer Polypropylene, 40% Talc Filled Data provided by Adell Plastics, Inc. |