Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 2.71 J/cm | 5.08 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP IN001 PA6.12 LNP* LUBRICOMP* IN001 is a compound based on Nylon 6/12 resin containing 2% Moly. Added feature of this grade is: Wear Resistant. |