Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 22.3 J/cm | 41.8 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics NORYL HS2000X PPE+PS PPE+PS blend. 17% Mineral reinforced. Non-brominated, non-chlorinated FR system. UL94 V0 and 5VA listing. UL746C f1. Radiant panel listing. Dielectric strength. Dimensional stability. Suitable for E.. |