Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 2.40 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
4.50 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256 |
PolyOne Gravi-Tech™ GRV-NY-112-W-NAT Polyamide 6 (Nylon 6) Information provided by PolyOne |
|||
Izod Impact, Unnotched | 2.40 J/cm | 4.50 ft-lb/in | ASTM D256 |
Network Polymers NPP 30-2000 TF40 Description: 40% Talc Filled Homopolymer PolypropyleneInformation provided by Network Polymers Inc. |
|||
Izod Impact, Unnotched | 2.40 J/cm | 4.50 ft-lb/in | ASTM D256 |
North Wood Plastics 60 HDPE + UNIFILL (20% Wood Fiber) Data provided by North Wood Plastics, Inc. UNIFILL-60 is a general purpose polyolefin compound compatible in both PP and HDPE. It is a masterbatch with 60% high quality pine wood flour filler. It.. |
|||
Izod Impact, Unnotched | 2.40 J/cm | 4.50 ft-lb/in | ASTM D256 |
Chevron Phillips Ryton® A-200 PPS Polyphenylene Sulfide
(discontinued **) Ryton® PPS is used in many electronic and automotive applications because of its high strength, favorable electrical properties, and high temperature stability.Data provided by the manufacturer.Sol.. |
|||
Izod Impact, Unnotched | 2.40 J/cm - NB | 4.50 ft-lb/in - NB | Average value: 6.74 J/cm Grade Count:91 |
Overview of materials for Polysulfone (PSU) This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone". Each property range of values reported is minimum and maximum values of appropriate MatWeb.. |
|||
Izod Impact, Unnotched | 2.40 J/cm @Temperature 23.0 °C |
4.50 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics Noryl TN240 PPE+PS (Asia Pacific) PPE+PS. Transparent. High flow, scratch resistant. Injection molding. Housewares and small appliances applications.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Unnotched | 2.40 J/cm @Thickness 3.17 mm |
4.50 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES Electrablend® ABS SS5 FR 5% Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel Fiber, 5% Filler by WeightFeatures: Electromagnetic Shielding (EMI) and Flame RetardantInformation provided by TP Compo.. |
|||
Izod Impact, Unnotched | 2.40 J/cm @Thickness 3.17 mm |
4.50 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES Electrablend® HDPE 04001 LE BK Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/Reinfor.Features: ESD Protection and ConductiveAppearance: BlackProcessing Method: ExtrusionInformation provided by .. |
|||
Izod Impact, Unnotched | 2.40 J/cm | 4.50 ft-lb/in | ASTM D256 |
Spartech SolarKote® /ABS Weatherable Sheet Description: Weatherable SheetSolarKote is a registered trademark of Atofina Chemicals, Inc..Information provided by Spartech. |
|||
Izod Impact, Unnotched | 2.40 J/cm | 4.50 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP STAT-KON Noryl_HMC1010 PPE+PS LNP* Stat-kon* Noryl_HMC1010 compound is a 10% Carbon fiber reinforced. Static dissipative. Nonbrominated, nonchlor- nated flame retardant system. UL94 V-1 rated. |
|||
Izod Impact, Unnotched | 2.40 J/cm @Thickness 3.17 mm |
4.50 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES Luriblend® POM HO TL20 BN042 Acetal Availability: North AmericaForms: PelletsAdditive: PTFE Lubricant(20%)Features: Lubricated and HomopolymerAppearance: Brown, Natural Color and RedInformation provided by TP Composites, Inc. |
|||
Izod Impact, Unnotched | 2.40 J/cm @Thickness 3.17 mm |
4.50 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES Electrablend® ABS 03011 BK MB Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/Reinfor.Features: Conductive, Electromagnetic Shielding (EMI) and Radio Frequency Shielding (RFI)Appearance: BlackIn.. |
|||
Izod Impact, Unnotched | 2.40 J/cm @Thickness 3.17 mm |
4.50 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES Electrablend® ABS SS15 BK MB 15% Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel Fiber, 15% Filler by WeightFeatures: Electromagnetic Shielding (EMI)Appearance: BlackInformation provided by TP Composi.. |
|||
Izod Impact, Unnotched | 2.40 J/cm | 4.50 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP IF003 PA 6/12 LNP THERMOCOMP* IF003 is a compound based on Nylon 6/12 resin containing 15% Glass Fiber. |
|||
Izod Impact, Unnotched | 2.40 J/cm | 4.50 ft-lb/in | ASTM D256 |
Westlake Plastics Propylux® CN-F Polypropylene (conductive) Non-sloughing, carbon-fiber-filled material with good chemical resistance, and high strength and stiffness and good temperature resistance to 215F. This material is light weight, easily machined an.. |
|||
Izod Impact, Unnotched | 2.40 J/cm @Thickness 3.17 mm |
4.50 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES Luriblend® POM HO TL20 BK Acetal Availability: North AmericaForms: PelletsAdditive: PTFE Lubricant(20%)Features: Lubricated and HomopolymerAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Izod Impact, Unnotched | 2.40 J/cm | 4.50 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP AX06472 ABS LNP* Thermocomp* AX06472 is a compound based on ABS containing a clay blend. |