Mechanical Properties Metric English Comments
Izod Impact, Unnotched 2.30 J/cm
4.31 ft-lb/in
ASTM D256
LNP NORYL® EXCP0112 PPS + Polyphenylene Ether, 40% Glass / Mineral Reinforcement  (discontinued **)
For applications requiring voltage resistance.Features: Corona resistantForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labele..
Izod Impact, Unnotched 2.30 - 2.70 J/cm

@Temperature 23.0 °C
4.31 - 5.06 ft-lb/in

@Temperature 73.4 °F
ISO R180
Fainplast Compounds RH 207/OP Rigid PVC, Antishock Extrusion
Medium antishock satined profiles
Izod Impact, Unnotched 2.30 J/cm
4.31 ft-lb/in
ASTM D256
Adell EA-18 Homopolymer Polypropylene, 40% Talc Filled
Data provided by Adell Plastics, Inc.
Izod Impact, Unnotched 2.30 J/cm
4.31 ft-lb/in
ASTM D4812
SABIC Innovative Plastics NORYL FE1410PW PPE+PS (Europe-Africa-Middle East)
Noryl* FE1410PW resin is a blend of polyphenylene Oxide (PPO) and polystyrene (PS) resin that contains 10% glass reinforcement. The resin is suitable for injection molding. Noryl FE1410PW resin has ..