Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 16.0 J/cm @Temperature 23.0 °C |
30.0 ft-lb/in @Temperature 73.4 °F |
DAM; ASTM D4812 |
DuPont Performance Polymers Minlon® 11C40 BKB086 Nylon 66
(Unverified Data**) Minlon® 11C40 BKB086 is a 40% mineral reinforced, heat stabilized, black polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Izod Impact, Unnotched | 16.0 J/cm @Temperature 23.0 °C |
30.0 ft-lb/in @Temperature 73.4 °F |
DAM; ASTM D4812 |
DuPont Performance Polymers Minlon® 12TA BKB124 Nylon 66
(Unverified Data**) Minlon® 12TA BKB124 is a 32% mineral reinforced, toughened, heat stabilized, black polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Izod Impact, Unnotched | 16.0 J/cm | 30.0 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP STAT-KON DX07323 PC+ABS (Asia Pacific) LNP* STAT-KON* DX07323 is a compound based on polycarbonate resin containing conductive fillers. Added features of this compound includes: ESD safe and excellent low-temperature impact performance, .. |
|||
Izod Impact, Unnotched | 16.0 J/cm | 30.0 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Xenoy® X2420 PC+POLYESTER (Asia Pacific) Xenoy*X2420 is a 10% glass filled, high flow, impact modified, injection moldable grade designed for high flow and impact strength. X2420 has enhanced melt flowability, impact ductility and broad co.. |
|||
Izod Impact, Unnotched | 16.0 J/cm @Temperature 23.0 °C |
30.0 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics LNP Stat-kon DS0029 PC LNP STAT-KON* DS0029 is a compound based on Polycarbonate resin containing Stainless Steel. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for t.. |
|||
Izod Impact, Unnotched | 16.0 J/cm | 30.0 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ PP 2268UX Heat Resistant Polypropylene DescriptionPolyfort® PP 2268UX is a UV stabilized, extra high flow unique high modulus, heat resistant polypropylene.Information provided by A. Schulman. |
|||
Izod Impact, Unnotched | 16.0 J/cm | 30.0 ft-lb/in | ASTM D256 |
A. Schulman PP 1259 Polypropylene Medium Impact Polypropylene DescriptionPolypropylene PP 1259 is a medium impact polypropylene with easier molding characteristics for thinner parts and longer flow distances. Lower molding pressures and heats often reduce war.. |
|||
Izod Impact, Unnotched | 16.0 J/cm | 30.0 ft-lb/in | ASTM D256 |
A. Schulman PP 1259 Polypropylene Medium Impact Polypropylene DescriptionPolypropylene PP 1259 is a medium impact polypropylene with easier molding characteristics for thinner parts and longer flow distances. Lower molding pressures and heats often reduce war.. |
|||
Izod Impact, Unnotched | 16.0 J/cm | 30.0 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ PP 2268UX Heat Resistant Polypropylene DescriptionPolyfort® PP 2268UX is a UV stabilized, extra high flow unique high modulus, heat resistant polypropylene.Information provided by A. Schulman. |
|||
Izod Impact, Unnotched | 16.0 J/cm | 30.0 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ PP 2268UX Heat Resistant Polypropylene DescriptionPolyfort® PP 2268UX is a UV stabilized, extra high flow unique high modulus, heat resistant polypropylene.Information provided by A. Schulman. |
|||
Izod Impact, Unnotched | 16.0 J/cm | 30.0 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FPP 1182 Talc Fortified Impact Resistant Polypropylene DescriptionPolyfort® FPP 1182 is a 20% talc fortified impact resistant polypropylene.Information provided by A. Schulman. |
|||
Izod Impact, Unnotched | 16.0 J/cm | 30.0 ft-lb/in | ASTM D256 |
A. Schulman PP 1259 Polypropylene Medium Impact Polypropylene DescriptionPolypropylene PP 1259 is a medium impact polypropylene with easier molding characteristics for thinner parts and longer flow distances. Lower molding pressures and heats often reduce war.. |
|||
Izod Impact, Unnotched | 16.0 J/cm | 30.0 ft-lb/in | ASTM D4812 |
Asahi Kasei Thermofil P-9900-1760 Unreinforced, Heat Stabilized, Impact Modified Information provided by Asahi Thermofil |
|||
Izod Impact, Unnotched | 16.0 J/cm @Temperature 23.0 °C |
30.0 ft-lb/in @Temperature 73.4 °F |
DAM; ASTM D4812 |
DuPont Performance Polymers Zytel® 77G43L BK031 Nylon 612
(Unverified Data**) Zytel® 77G43L BK031 is a 43% glass fiber reinforced, black polyamide 612 resin for injection molding.Information provided by DuPont Performance Polymers |