Mechanical Properties Metric English Comments
Izod Impact, Unnotched 2.02882 - 2.1356 J/cm

@Temperature -18.0 - -18.0 °C
3.80081 - 4.0009 ft-lb/in

@Temperature -0.400 - -0.400 °F
Average value: 2.06 J/cm Grade Count:3
Overview of materials for Polypropylene, Extrusion Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Extrusion Grade". Each property range of values reported is minimum and maximum values of..