Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 1.71 J/cm @Thickness 3.17 mm |
3.20 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Niche Polymer PA66MIBK Nylon 66, Medium Impact Information provided by Niche Polymer |
|||
Izod Impact, Unnotched | 1.71 J/cm @Thickness 3.17 mm |
3.20 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Niche Polymer PA66MIN Nylon 66, Medium Impact Information provided by Niche Polymer |
|||
Izod Impact, Unnotched | 1.71 J/cm @Thickness 3.18 mm |
3.20 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
LNP Konduit® OTF-212-11 Polyphenylene Sulfide, Proprietary Filler
(discontinued **) Features: Thermally ConductiveForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades ar.. |
|||
Izod Impact, Unnotched | 1.71 J/cm | 3.20 ft-lb/in | ASTM D256 |
A. Schulman ComAlloy Hiloy® 283 PPO Alloy, Glass Reinforced Data provided by the manufacturer, ComAlloy International Company.35% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Izod Impact, Unnotched | 1.71 J/cm | 3.20 ft-lb/in | ASTM D256 |
A. Schulman ComAlloy Hiloy® 284 PPO Alloy, Glass/Graphite Reinforced Data provided by the manufacturer, ComAlloy International Company.50% Glass/Graphite Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Izod Impact, Unnotched | 1.71 J/cm @Temperature -40.0 °C |
3.20 ft-lb/in @Temperature -40.0 °F |
|
Chevron Phillips Ryton® R10 7006A PPS Polyphenylene Sulfide
(discontinued **) Ryton® PPS is used in many electronic and automotive applications because of its high strength, favorable electrical properties, and high temperature stability.Data provided by the manufacturer.Sol.. |
|||
Izod Impact, Unnotched | 1.71 J/cm @Thickness 3.18 mm |
3.20 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
LNP Konduit® OTF-212-11 BK8-115 Polyphenylene Sulfide, Proprietary Filler
(discontinued **) Features: Thermally ConductiveForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades ar.. |