Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 1.60 - 5.34 J/cm | 3.00 - 10.0 ft-lb/in | Average value: 2.38 J/cm Grade Count:11 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 10% Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 10% Carbon Fiber Filled". Specific grades with carbon fiber conte.. |
|||
Izod Impact, Unnotched | 1.60 J/cm | 3.00 ft-lb/in | Average value: 1.60 J/cm Grade Count:10 |
Overview of materials for Polytetrafluoroethylene (PTFE), Glass Filled, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Glass Filled, Molded". Each property range of values reported is minimum.. |
|||
Izod Impact, Unnotched | 1.60 J/cm | 3.00 ft-lb/in | J/cm²; ISO 180A |
Solvay Specialty Polymers Ryton® R-7-120BL Polyphenylene Sulfide Compound
(Unverified Data**) Black Polyphenylene Sulfide CompoundRyton® R-7-120BL is an advanced glass/mineral filled polyphenylene sulfide compound developed to provide good weldline strength and low maintenance molding using.. |
|||
Izod Impact, Unnotched | 1.60 J/cm | 3.00 ft-lb/in | ASTM D256 |
Chevron Phillips Ryton® R10-110BL Polyphenylene Sulfide Compound
(discontinued **) Black Polyphenylene Sulfide CompoundRyton® R10-110BL is a glass and mineral filled polyphenylene sulfide compound which provides a good combination of mechanical and electrical properties.Applicati.. |
|||
Izod Impact, Unnotched | 1.60 - 2.00 J/cm @Temperature 23.0 °C |
3.00 - 3.75 ft-lb/in @Temperature 73.4 °F |
ISO R180 |
Fainplast Compounds RH 225 Rigid PVC, Antishock Extrusion Antishock pipes and profiles |
|||
Izod Impact, Unnotched | 1.60 J/cm @Thickness 3.17 mm |
3.00 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Ineos ABS Lustran® SAN Sparkle Highest-Clarity |
|||
Izod Impact, Unnotched | 1.60 J/cm | 3.00 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics ULTEM 4000 PEI Glass fiber, PTFE, and Graphite filled, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 listing. |
|||
Izod Impact, Unnotched | 1.60 J/cm @Thickness 3.17 mm |
3.00 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES Electrablend® ABS CF10 10% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 10% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Izod Impact, Unnotched | 1.60 J/cm @Thickness 3.17 mm |
3.00 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES Electrablend® ABS CF5 5% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 5% Filler by WeightAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Izod Impact, Unnotched | 1.60 J/cm | 3.00 ft-lb/in | ASTM D256 |
Daikin POLYFLON F-104 PTFE Fine Powder Processing Methods: Paste extrusion, calendering.Applications: Unsintered tape, sealing tape, low specific gravity tape, tape for wrapping flat cables, tubes.Information provided by Daikin Industrie.. |
|||
Izod Impact, Unnotched | 1.60 J/cm | 3.00 ft-lb/in | ASTM D256 |
Daikin POLYFLON M-12 PTFE Molding Powder, Fine Cut Fine cut powder.Processing Methods: Compression molding.Features: Useful in making products requiring fine texture, especially insulation skiving tapes. Also allows uniform mixing of inorganic fill.. |
|||
Izod Impact, Unnotched | 1.60 J/cm | 3.00 ft-lb/in | ASTM D256 |
Daikin POLYFLON M-391 PTFE Molding Powder, Free Flow Free flow powder.Processing Methods: Compression molding and automatic or semi-automatic compression molding.Features: Used if concerned about insufficient molding pressure for flat sheets.Informati.. |
|||
Izod Impact, Unnotched | 1.60 J/cm | 3.00 ft-lb/in | ASTM D256 |
Daikin POLYFLON MG-1030 PTFE 15% Glass Fiber Filled Molding Powder 15% glass fiber filled. High wear resistance, low friction, good electrical properties.Applications: Mechanical and electrical service. Available in all forms (e.g. bearings, gaskets, valve seats,.. |
|||
Izod Impact, Unnotched | 1.60 J/cm | 3.00 ft-lb/in | ASTM D256 |
A. Schulman ComAlloy Hiloy® 758 Carbon Fiber Reinforced, Flow Enhanced, PPS Alloy Data provided by the manufacturer, ComAlloy International Company.40% Carbon Fiber Reinforced. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has b.. |
|||
Izod Impact, Unnotched | 1.60 - 5340 J/cm | 3.00 - 10000 ft-lb/in | Average value: 4.74 J/cm Grade Count:42 |
Overview of materials for Polytrimethylene Terephthalate (PTT) This property data is a summary of similar materials in the MatWeb database for the category "Polytrimethylene Terephthalate (PTT)". Each property range of values reported is minimum and maximum val.. |