Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 14.0 J/cm | 26.2 ft-lb/in | ASTM D256 |
PolyOne OnForce™ LFT NN-30 LGF/000 Natural Polyamide 66 (Nylon 66) PolyOne's Long Fiber Thermoplastic (LFT) compounds are formulated for demanding applications which require high stiffness and good impact such as metal replacement or other structural applications. .. |
|||
Izod Impact, Unnotched | 14.0 J/cm | 26.2 ft-lb/in | ASTM D256 |
PolyOne OnForce™ LFT UR-40 LGF/000 Natural Polyurethane, Unspecified (PUR, Unspecified) PolyOne's Long Fiber Thermoplastic (LFT) compounds are formulated for demanding applications which require high stiffness and good impact such as metal replacement or other structural applications. .. |
|||
Izod Impact, Unnotched | 14.0 J/cm | 26.2 ft-lb/in | ASTM D4812 |
Premix Premi-Glas® 2143-24 CR-SX Fiberglass Reinforced Thick Molding Compound Premi-Glas® 2143-24 CR-SX is a fiberglass reinforced thermoset thick molding compound for electrical and flame retardant applications.Key features and benefits are:TMC compounding process preserves.. |
|||
Izod Impact, Unnotched | 14.0 J/cm | 26.2 ft-lb/in | ASTM D4812 |
Premix Premi-Glas® 2143-24 CR-SX-HT Fiberglass Reinforced Thick Molding Compound Premi-Glas® 2143-24 CR-SX is a fiberglass reinforced thermoset thick molding compound for electrical and flame retardant applications.Key features and benefits are:TMC compounding process preserves.. |
|||
Izod Impact, Unnotched | 14.0 J/cm | 26.2 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Amodel® AT-6130 HS Polyphthalamide (PPA), 30% Glass Fiber (Dry) Amodel® AT-6130 HS is a 30% glass-reinforced, toughened polyphthalamide (PPA) resin that has more elongation than other 30% glass-reinforced grades of Amodel® resin. This grade was developed f.. |
|||
Izod Impact, Unnotched | 14.0 J/cm | 26.2 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP HX03408 PA11 LNP* Thermocomp* HX03408 is a compound based on Nylon 11 containing Proprietary Fillers. Added feature includes: Clean Compound System |
|||
Izod Impact, Unnotched | 14.0 J/cm | 26.2 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics NORYL LTA1350 PPE+PS Noryl* LTA1350 is an unfilled, injection moldable grade. Designed for improved long term heat aging, this resin also uses non-chlorinated, non-brominated FR additives to achieve a V0 UL94 rating. No.. |
|||
Izod Impact, Unnotched | 14.0 J/cm | 26.2 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics NORYL LTA1350 PPE+PS (Asia Pacific) Noryl* LTA1350 is an unfilled, injection moldable grade. Designed for improved long term heat aging, this resin also uses non-chlorinated, non-brominated FR additives to achieve a V0 UL94 rating. No.. |
|||
Izod Impact, Unnotched | 14.0 J/cm | 26.2 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics NORYL LTA5020 PPE+PS Noryl* LTA5020 is an unfilled, injection moldable grade. Designed for improved long term heat aging, this resin also uses non-chlorinated, non-brominated FR additives to achieve a V0 UL94 rating. No.. |
|||
Izod Impact, Unnotched | 14.0 J/cm | 26.2 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP STAT-LOY W3000XXJ PBT LNP* STAT-LOY* W3000XXJ is a compound based on PBT. Added features of this grade include: Anti-Stat, Colorable, Healthcare |
|||
Izod Impact, Unnotched | 14.0 J/cm | 26.2 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics NORYL LTA1350 PPE+PS (Europe-Africa-Middle East) Noryl* LTA1350 is an unfilled, injection moldable grade. Designed for improved long term heat aging, this resin also uses non-chlorinated, non-brominated FR additives to achieve a V0 UL94 rating. No.. |