Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 133 - 160 J/cm @Thickness 3.17 mm |
249 - 300 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Diamond Polymers NYLON 6615 Black, Super Tough Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |