Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 11.35 J/cm | 21.25 ft-lb/in | ASTM D256-93 |
Compuestos Dominicanos Polycom BD-320699 PVC Compound The polycom BD series are compounds for blow molding of PVC bottles suitable for the packaging of edible oil, water, cleaning products and lubricants. These compounds produce bottles with high clar.. |
|||
Izod Impact, Unnotched | 11.35 J/cm | 21.25 ft-lb/in | ASTM D256-93 |
Compuestos Dominicanos Polycom BD-330699 PVC Compound The polycom BD series are compounds for blow molding of PVC bottles suitable for the packaging of edible oil, water, cleaning products and lubricants. These compounds produce bottles with high clar.. |
|||
Izod Impact, Unnotched | 11.35 J/cm | 21.25 ft-lb/in | ASTM D256-93 |
Compuestos Dominicanos Polycom BD-340599 PVC Description: The polycom BD series are compounds for the blow molding of PVC bottles suitable for the packing of edible oil, water, cleansing products and lubricants. These compounds produce bottles.. |
|||
Izod Impact, Unnotched | 11.35 J/cm | 21.25 ft-lb/in | ASTM D256-93 |
Compuestos Dominicanos Polycom BD-220699 PVC Compound The polycom BD series are compounds for blow molding of PVC bottles suitable for the packaging of edible oil, water, cleaning products and lubricants. These compounds produce bottles with high clar.. |