Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 10.35 J/cm | 19.39 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP UFL36S PPA LNP LUBRICOMP* UFL36S is a compound based on Polyphthalamide resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Heat Stabilized, Wear Resistant, Bearing Grade. |
|||
Izod Impact, Unnotched | 10.35 J/cm | 19.39 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP UFL36SXP PPA LNP LUBRICOMP* UFL36SXP is a compound based on Polyphthalamide resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Heat Stabilized, Wear Resistant. |