Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 9.45 J/cm | 17.7 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP DBP32EI PC LNP* Lubricomp* DBP32EI is a compound based on Polycarbonate resin containing 15% PTFE/Silicone and 10% Glass Bead. Added features of this material include: Internally Lubricated. |
|||
Izod Impact, Unnotched | 9.45 J/cm | 17.7 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP DBP32EI PC (Asia Pacific) LNP* Lubricomp* DBP32EI is a compound based on Polycarbonate resin containing PTFE, Carbon Fiber. Added features of this material include: Electrically Conductive, Internally Lubricated. |
|||
Izod Impact, Unnotched | 9.45 J/cm | 17.7 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP RCP36 PA 66 LNP LUBRICOMP* RCP36 is a compound based on Nylon 66 resin containing 30% Carbon Fiber, 15% PTFE/Silicone. Added features of this material include: Electrically Conductive, Wear Resistant. |
|||
Izod Impact, Unnotched | 9.45 J/cm | 17.7 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP RCP36 PA 66 (Asia Pacific) LNP LUBRICOMP* RCP36 is a compound based on Nylon 66 resin containing Silicone, PTFE, Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Izod Impact, Unnotched | 9.45 J/cm | 17.7 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP RCP36 PA 66 (Europe-Africa-Middle East) LNP LUBRICOMP* RCP36 is a compound based on Nylon 66 resin containing Carbon Fiber, Silicone, PTFE. Added features of this material include: Electrically Conductive. |
|||
Izod Impact, Unnotched | 9.47 J/cm | 17.7 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP STAT-KON RE004MPC PA 66 LNP* STAT-KON* RE004MPC is a compound based on Nylon 66 resin containing 20% Milled Carbon Fiber. Added features of this material are: Exceptional Processing, Clean Compound System, Electrically C.. |
|||
Izod Impact, Unnotched | 9.47 J/cm | 17.7 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP DX06411H PC LNP* THERMOCOMP* DX06411H is a compound based on Polycarbonate resin containing 20% Glass Fiber. Added features of this material include: Easy Molding, Mold Release, Healthcare. |