Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 8.21 J/cm | 15.4 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP DFL12 PC LNP* Lubricomp* DFL12 is a compound based on Polycarbonate resin containing 10% Glass Fiber and 5% PTFE. Added features include: Internally Lubricated. |
|||
Izod Impact, Unnotched | 8.20 J/cm | 15.4 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Valox® 8032UX PBT+PET (Europe-Africa-Middle East) VALOX 8032UX is a 30% glass fibre reinforced, UV stabilized PBT+PET blend with excellent surface finish. This grade is VALOX 8032U with improved weathering resistance. Applications: appliance housin.. |
|||
Izod Impact, Unnotched | 8.21 J/cm @Temperature 23.0 °C |
15.4 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics LNP Thermocomp DFZ22E PC LNP* Thermocomp* DFZ22E is a compound based on Polycarbonate with Glass and Milled Fiber. Characteristics of this products is Easy Molding.This data was supplied by SABIC-IP for the Americas region.. |
|||
Izod Impact, Unnotched | 8.23 J/cm | 15.4 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP IF004 PA 6/12 (Asia Pacific) LNP* Thermocomp* IF004 is a compound based on Nylon 6/12 resin containing Glass Fiber. |
|||
Izod Impact, Unnotched | 8.22 J/cm | 15.4 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP PX12419 PA 6 LNP* THERMOCOMP* PX12419 is a compound based on Nylon 6 containing Carbon Fiber. Added features of this grade include: Electrically Conductive. |