Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 7.30 J/cm | 13.7 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Ixef® 1028 Polyarylamide (PARA)
(discontinued **) Ixef 1028 is a laser printable, 50% glass-fiber reinforced polyarylamide which exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance. - Black: Ixef 1028.. |
|||
Izod Impact, Unnotched | 7.31 J/cm | 13.7 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRILOY RF203AXH PA 66 LNP* LUBRILOY* RF203AXH is a compound based on Nylon 66 resin containing 15% Glass Fiber, Proprietary Lubricant. Added features of this material include: Wear Resistant, Healthcare. |
|||
Izod Impact, Unnotched | 7.30 J/cm | 13.7 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Valox® 412 PBT (Europe-Africa-Middle East) VALOX 412 is 20% glass reinforced PBT injection moulding resin. Applications: Spotlights, appliance housings and handles. |
|||
Izod Impact, Unnotched | 7.30 J/cm | 13.7 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Valox® 865 PBT (Europe-Africa-Middle East) VALOX 865 is a 30% glass fibre reinforced, non blooming flame retardant PBT+PET blend with an excellent surface appearance. Applications: External housings, steam irons, appliance housings and light.. |
|||
Izod Impact, Unnotched | 7.32 J/cm | 13.7 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP STAT-KON DX09315C PC (Asia Pacific) LNP* Stat-Kon* DX09315C is carbon fiber filled polycarbonate composite with good flow ability, and high level of cleanliness for the most demanding application. A unique feature of this material is .. |
|||
Izod Impact, Unnotched | 7.32 J/cm | 13.7 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP STAT-KON REL33 PA 66 LNP STAT-KON* REL33 is a compound based on Nylon 66 resin containing 15% Carbon Fiber, 15% PTFE. Added features of this material include: Electrically Conductive, Wear Resistant. |
|||
Izod Impact, Unnotched | 7.29 J/cm | 13.7 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP DX06412H PC LNP* THERMOCOMP* DX06412H is a compound based on Polycarbonate resin containing 30% Glass Fiber. Added features of this material include: Easy Molding, Mold Release. |
|||
Izod Impact, Unnotched | 7.29 J/cm | 13.7 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP DX06412H PC (Asia Pacific) LNP* Thermocomp* DX06412H is a compound based on Polycarbonate resin containing Glass Fiber. Added features of this material include: Easy Molding, Mold Release. |
|||
Izod Impact, Unnotched | 7.29 J/cm @Temperature 23.0 °C |
13.7 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics LNP Thermocomp KB002 Acetal Copoly LNP* Thermocomp* KB002 is a compound based on Acetal Copolymer resin containing Glass Bead.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Unnotched | 7.31 J/cm | 13.7 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP RF006EXZ PA 66 LNP THERMOCOMP* RF006EXZ is a compound based on Nylon 66 resin containing 30% Glass Fiber. Added features of this material include: Easy Molding. |
|||
Izod Impact, Unnotched | 7.29 J/cm @Temperature 23.0 °C |
13.7 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics LNP Thermocomp KB002 Acetal Copoly (Asia Pacific) LNP* Thermocomp* KB002 is a compound based on Acetal Copolymer resin containing Glass Bead.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Unnotched | 7.31 J/cm | 13.7 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP RF006ESZ PA 66 LNP THERMOCOMP* RF006ESZ is a compound based on Nylon 66 resin containing 30% Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized. |
|||
Izod Impact, Unnotched | 7.29 J/cm | 13.7 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP RF0069XZ PA 66 LNP THERMOCOMP* RF0069XZ is a compound based on Nylon 66 resin containing 30% Glass Fiber. Added features of this material include: Flame Retardant. |