Polymer Property : Izod Impact, Unnotched = 1.38 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched 0.735 J/cm
1.38 ft-lb/in
ASTM D256
Hyosung Topilene C500H PP
C500H Butene Random CopolymerApplications: FilmCharacteristics:Excellent transparency & glossLow sealing temperatureHigh hot-tack strengthGood stiffnessInformation provided by Hyosung Corporation
Izod Impact, Unnotched 0.735 J/cm
1.38 ft-lb/in
ASTM D256
Hyosung Topilene C600H PP
C600H Film Grade Butane Random CopolymerApplications: Sealable CPP/OPPCharacteristics:Very low sealSlip propertyTransparencyInformation provided by Hyosung Corporation
Izod Impact, Unnotched 0.735 J/cm
1.38 ft-lb/in
ASTM D256
Hyosung Topilene C600HF PP
C600HF Film Grade Butane Random CopolymerApplications: Sealable CPP/OPPCharacteristics:Low sealSlip propertyTransparencyInformation provided by Hyosung Corporation
Izod Impact, Unnotched 0.735 J/cm
1.38 ft-lb/in
ASTM D256
Hyosung Topilene J742 PP
J742 Injection Impact CopolymerApplications: Large articles:Washing M/C partsElectric applianceIndustrial applianceCharacteristics:Medium impactHigh stiffnessInformation provided by Hyosung Corporat..