Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 0.534 J/cm @Thickness 3.17 mm |
1.00 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Niche Polymer PA66BK Nylon 66 Information provided by Niche Polymer |
|||
Izod Impact, Unnotched | 0.534 J/cm @Thickness 3.17 mm |
1.00 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Niche Polymer PPCT20BK Copolymer PP, 20% Talc Filled Information provided by Niche Polymer |
|||
Izod Impact, Unnotched | 0.534 - 2.94 J/cm | 1.00 - 5.51 ft-lb/in | Average value: 1.67 J/cm Grade Count:19 |
Overview of materials for Polystyrene, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Glass Filled". Each property range of values reported is minimum and maximum values of appr.. |
|||
Izod Impact, Unnotched | 0.534 - 5340 J/cm | 1.00 - 10000 ft-lb/in | Average value: 9.81 J/cm Grade Count:19 |
Overview of materials for Polypropylene with 20% Calcium Carbonate (CaCO3) Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Calcium Carbonate (CaCO3) Filler". Each property range of values reported is mini.. |
|||
Izod Impact, Unnotched | 0.534 - 13.0 J/cm | 1.00 - 24.4 ft-lb/in | Average value: 5.23 J/cm Grade Count:6 |
Overview of materials for Polyphenylene Sulfide (PPS); Molded This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS); Molded". Each property range of values reported is minimum and maximum valu.. |
|||
Izod Impact, Unnotched | 0.534 J/cm - NB | 1.00 ft-lb/in - NB | Average value: 9.53 J/cm Grade Count:9 |
Overview of materials for Nylon 66, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Unreinforced". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Izod Impact, Unnotched | 0.534 J/cm @Temperature -40.0 °C |
1.00 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Spartech SolarKote® /ABS Weatherable Sheet Description: Weatherable SheetSolarKote is a registered trademark of Atofina Chemicals, Inc..Information provided by Spartech. |
|||
Izod Impact, Unnotched | 0.534 J/cm @Temperature -40.0 °C |
1.00 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Spartech SP-9070 ABS/PVC Flame Retardant Sheet Description: Flame Retardant SheetInformation provided by Spartech. |
|||
Izod Impact, Unnotched | 0.534 J/cm | 1.00 ft-lb/in | ASTM D256 |
Ensinger Tecaform™ AH ID Metal Detectable Acetal Copolymer (POM) TECAFORM™ AH ID is the fist commercially available acetal that is fully detectable by standard metal detection equipment. Exhibiting excellent machinability and a good combination of physical prop.. |