Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 0.490 J/cm | 0.918 ft-lb/in | ASTM D256 |
North Wood Plastics Polypropylene with 60% Wood Fiber, Extrusion Grade Data provided by North Wood Plastics, Inc. |
|||
Izod Impact, Unnotched | 0.490 J/cm | 0.918 ft-lb/in | ASTM D256 |
Hyosung Topilene B301 PP B301 HomopolymerApplications:Thermoforming sheetsCharacteristics:High melt tensionDimensional stabilityGood optical propertyInformation provided by Hyosung Corporation |
|||
Izod Impact, Unnotched | 0.490 J/cm | 0.918 ft-lb/in | ASTM D256 |
Hyosung Topilene C600 PP C600 Film Grade Butane Random CopolymerApplications: Metallizing CPPCharacteristics:Al bonding strengthHigh glossInformation provided by Hyosung Corporation |
|||
Izod Impact, Unnotched | 0.490 J/cm | 0.918 ft-lb/in | ASTM D256 |
Hyosung Topilene C600MU PP C600MU Butene Random CopolymerApplications: FilmCharacteristics:Excellent transparency & glossLow sealing temperatureHigh hot-tack strengthGood stiffnessInformation provided by Hyosung Corporation |
|||
Izod Impact, Unnotched | 0.490 J/cm @Temperature -10.0 °C |
0.918 ft-lb/in @Temperature 14.0 °F |
ASTM D256 |
Hyosung Topilene J640 PP J640 Injection Impact CopolymerApplications:General purposeBattery caseElectric applianceCharacteristics:Medium ImpactFlowabilityInformation provided by Hyosung Corporation |
|||
Izod Impact, Unnotched | 0.490 J/cm @Temperature -10.0 °C |
0.918 ft-lb/in @Temperature 14.0 °F |
ASTM D256 |
Hyosung Topilene J640U PP J640U Injection Impact CopolymerApplications:General purposeBattery caseElectric applianceCharacteristics:Medium ImpactFlowabilityWeatherabilityInformation provided by Hyosung Corporation |
|||
Izod Impact, Unnotched | 0.490 J/cm @Temperature -10.0 °C |
0.918 ft-lb/in @Temperature 14.0 °F |
ASTM D256 |
Hyosung Topilene J642 PP J642 Injection Impact CopolymerApplications:Washing M/C partsElectric applianceCharacteristics:Medium impactHigh stiffnessInformation provided by Hyosung Corporation |
|||
Izod Impact, Unnotched | 0.490 J/cm | 0.918 ft-lb/in | ASTM D256 |
Hyosung Topilene R500F PP R500F Block CopolymerApplications: Retort CPPCharacteristics:Excellent impact strengthFish eye freeHeat resistanceGood clarityInformation provided by Hyosung Corporation |
|||
Izod Impact, Unnotched | 0.490 J/cm | 0.918 ft-lb/in | ASTM D256 |
Hyosung Topilene R500S PP R500S Block CopolymerApplications: Retort CPPCharacteristics:Excellent impact strengthFish eye freeHeat resistanceGood clarityInformation provided by Hyosung Corporation |
|||
Izod Impact, Unnotched | 0.490 J/cm | 0.918 ft-lb/in | ASTM D256 |
Hyosung Topilene R801H PP R801H Injection Random CopolymerApplications:High transparent productLarge articlesCharacteristics:High transparencyStiffnessInformation provided by Hyosung Corporation |
|||
Izod Impact, Unnotched | 0.490 J/cm @Thickness 3.17 mm |
0.918 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samyang Tribit® 1500GN15 Polybutylene Terephthalate, 15% Glass Reinforced, Flame Retardant Characteristics:G/F reinforcedFlame retardantHeat and Impact resistantApplications:AutomotiveConnectorGearOutdoor handleIgnition systemElectronicConnectorGas valveCoil bobbinSwitch caseRelay caseO/A.. |