Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 0.480 J/cm - NB | 0.899 ft-lb/in - NB | Average value: 7.02 J/cm Grade Count:48 |
Overview of materials for Acetal Copolymer, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Unreinforced". Each property range of values reported is minimum and maximum values of.. |
|||
Izod Impact, Unnotched | 0.480 J/cm | 0.899 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP KG002 Acetal Copolymer LNP* LUBRICOMP* KG002 is a compound based on Acetal Copolymer resin containing 10% Graphite. Added feature of this material is: Wear Resistant. |
|||
Izod Impact, Unnotched | 0.480 J/cm | 0.899 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP KG002 Acetal Copolymer (Asia Pacific) LNP* Lubricomp* KG002 is a compound based on Acetal Copolymer resin containing Graphite Powder. Added features of this material include: Internally Lubricated. |
|||
Izod Impact, Unnotched | 0.480 J/cm | 0.899 ft-lb/in | ASTM D256 |
Ensinger TECAPRO™ MT Medical Grade Polypropylene (PP) TECAPRO™ MT is an FDA approved homopolymer polypropylene based material with exceptionally low residual stress to facilitate the fabrication of dimensionally stable parts with varying cross section.. |