Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 0.343 J/cm @Temperature -10.0 °C |
0.643 ft-lb/in @Temperature 14.0 °F |
ASTM D256 |
Hyosung Topilene HJ740 PP HJ740 High Isostatic PP Impact CopolymerApplications:CompoundingElectric applianceAutomobile partsCharacteristics:High stiffnessHeat resistanceMedium impactInformation provided by Hyosung Corporatio.. |
|||
Izod Impact, Unnotched | 0.343 J/cm @Temperature -10.0 °C |
0.643 ft-lb/in @Temperature 14.0 °F |
ASTM D256 |
Hyosung Topilene J440F PP J440F Block CopolymerApplications: Retort CPPCharacteristics:Excellent impact strengthFish eye freeHeat resistanceGood clarityInformation provided by Hyosung Corporation |
|||
Izod Impact, Unnotched | 0.343 J/cm | 0.643 ft-lb/in | ASTM D256 |
Hyosung Topilene J801R PP J801R Injection Special Purpose GradeApplications: Electric home applianceCharacteristics:High stiffnessLong-term heat resistanceInformation provided by Hyosung Corporation |
|||
Izod Impact, Unnotched | 0.343 J/cm @Temperature -10.0 °C |
0.643 ft-lb/in @Temperature 14.0 °F |
ASTM D256 |
Hyosung Topilene J945 PP J945 Injection Impact CopolymerApplications: Very large articles:Washing M/C partsIndustrial applianceCharacteristics:High flowabilityHigh stiffnessInformation provided by Hyosung Corporation |
|||
Izod Impact, Unnotched | 0.343 J/cm | 0.643 ft-lb/in | ASTM D256 |
Hyosung Topilene J801 PP J801 Injection Special Purpose GradeApplications:Disposable syringeTransparent productCharacteristics:TransparencyHigh stiffnessInformation provided by Hyosung Corporation |