Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Izod Impact, Unnotched = 0.562 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched 0.300 - 34.2 J/cm
0.562 - 64.1 ft-lb/in
Average value: 2.28 J/cm Grade Count:88
Overview of materials for PVC, Extruded
This property data is a summary of similar materials in the MatWeb database for the category "PVC, Extruded". Each property range of values reported is minimum and maximum values of appropriate MatW..
Izod Impact, Unnotched 0.300 - 0.700 J/cm

@Temperature 23.0 °C
0.562 - 1.31 ft-lb/in

@Temperature 73.4 °F
ISO R180
Fainplast Compounds RK 335/1 Rigid PVC, Extrusion Lead Free
Profiles
Izod Impact, Unnotched 0.300 J/cm
0.562 ft-lb/in
ASTM D256
Equate EMDA-8920 HDPE Injection Molding Resin
EMDA-8920 is a high density copolymer polyethylene resin designed for injection molding applications which require excellent toughness and gloss.Applications: EMDA-8920 is a high density copolymer p..
Izod Impact, Unnotched 0.300 - 5340 J/cm
0.562 - 10000 ft-lb/in
Average value: 0.300 J/cm Grade Count:3
Overview of materials for High Density Polyethylene (HDPE), Injection Molded
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Injection Molded". Each property range of values reported is minimum a..
Copyright © lookpolymers.com All Rights Reserved