Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 5.10 - 5.10 J/cm @Temperature -40.0 - -40.0 °C |
9.55 - 9.55 ft-lb/in @Temperature -40.0 - -40.0 °F |
Average value: 5.10 J/cm Grade Count:1 |
Overview of materials for Polyethylene Terephthalate (PET), 40% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 40% Glass Reinforced". Specific grades with glass content between 35% .. |