Mechanical Properties Metric English Comments
Izod Impact, Unnotched 2.40 - 2.80 J/cm

@Temperature 23.0 °C
4.50 - 5.25 ft-lb/in

@Temperature 73.4 °F
ISO R180
Fainplast Compounds RH 210/W Rigid PVC, Antishock Extrusion
Various antishock profiles
Izod Impact, Unnotched 2.40 - 2.80 J/cm

@Temperature 23.0 °C
4.50 - 5.25 ft-lb/in

@Temperature 73.4 °F
ISO R180
Fainplast Compounds RH 325 Rigid PVC, Antishock Extrusion
Antishock furniture profiles