Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 0.392 - 15.9 J/cm | 0.735 - 29.8 ft-lb/in | Average value: 9.00 J/cm Grade Count:8 |
Overview of materials for Polypropylene, Extrusion Grade This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Extrusion Grade". Each property range of values reported is minimum and maximum values of.. |