Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 0.801 - 10.7 J/cm | 1.50 - 20.0 ft-lb/in | Average value: 3.62 J/cm Grade Count:22 |
Overview of materials for Polystyrene, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Impact Modified". Each property range of values reported is minimum and maximum values of a.. |
|||
Izod Impact, Unnotched | 2.67 - 10.7 J/cm | 5.00 - 20.0 ft-lb/in | Average value: 7.12 J/cm Grade Count:6 |
Overview of materials for Acetal Copolymer, Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Mineral Filled". Each property range of values reported is minimum and maximum values .. |
|||
Izod Impact, Unnotched | 4.81 - 10.7 J/cm | 9.00 - 20.0 ft-lb/in | Average value: 7.47 J/cm Grade Count:8 |
Overview of materials for Polycarbonate, Aramid Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Aramid Fiber Reinforced". Each property range of values reported is minimum and maximum v.. |
|||
Izod Impact, Unnotched | 4.81 - 10.7 J/cm | 9.00 - 20.0 ft-lb/in | Average value: 7.47 J/cm Grade Count:19 |
Overview of materials for Nylon 6, Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum and max.. |
|||
Izod Impact, Unnotched | 6.41 - 10.7 J/cm | 12.0 - 20.0 ft-lb/in | Average value: 8.45 J/cm Grade Count:13 |
Overview of materials for Nylon 66, 30% Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 30% Carbon Fiber Filled". Specific grades with carbon fiber content between 25% and 34% are in.. |
|||
Izod Impact, Unnotched | 3.20 - 10.7 J/cm | 6.00 - 20.0 ft-lb/in | Average value: 6.85 J/cm Grade Count:45 |
Overview of materials for Nylon 66, Carbon Fiber/PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Carbon Fiber/PTFE Filled". Each property range of values reported is minimum and maximum value.. |
|||
Izod Impact, Unnotched | 4.81 - 10.7 J/cm | 9.00 - 20.0 ft-lb/in | Average value: 8.33 J/cm Grade Count:15 |
Overview of materials for Nylon 66, Stainless Steel Filled; EMI Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Stainless Steel Filled; EMI Grade". Each property range of values reported is minimum and maxi.. |
|||
Izod Impact, Unnotched | 3.79 - 10.7 J/cm | 7.10 - 20.0 ft-lb/in | Average value: 7.37 J/cm Grade Count:10 |
Overview of materials for Nylon 610, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 610, Carbon Fiber Filled". Each property range of values reported is minimum and maximum values of.. |
|||
Izod Impact, Unnotched | 2.40 - 10.7 J/cm | 4.50 - 20.0 ft-lb/in | Average value: 6.27 J/cm Grade Count:31 |
Overview of materials for Nylon 612, Carbon Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Carbon Fiber Filler". Each property range of values reported is minimum and maximum values of.. |
|||
Izod Impact, Unnotched | 5.34 - 10.7 J/cm | 10.0 - 20.0 ft-lb/in | Average value: 8.12 J/cm Grade Count:7 |
Overview of materials for Nylon 11 + Carbon Fiber This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11 + Carbon Fiber". Each property range of values reported is minimum and maximum values of approp.. |
|||
Izod Impact, Unnotched | 1.10 - 10.7 J/cm | 2.06 - 20.0 ft-lb/in | Average value: 6.54 J/cm Grade Count:14 |
Overview of materials for Nylon 12, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, Carbon Fiber Filled". Each property range of values reported is minimum and maximum values of .. |
|||
Izod Impact, Unnotched | 2.14 - 10.7 J/cm | 4.00 - 20.0 ft-lb/in | Average value: 6.83 J/cm Grade Count:5 |
Overview of materials for PC/ABS + Stainless Steel This property data is a summary of similar materials in the MatWeb database for the category "PC/ABS + Stainless Steel". Each property range of values reported is minimum and maximum values of appro.. |
|||
Izod Impact, Unnotched | 1.87 - 10.7 J/cm | 3.50 - 20.0 ft-lb/in | Average value: 4.43 J/cm Grade Count:13 |
Overview of materials for Polypropylene Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene Glass Bead Filled". Each property range of values reported is minimum and maximum values o.. |
|||
Izod Impact, Unnotched | 2.14 - 10.7 J/cm | 4.00 - 20.0 ft-lb/in | Average value: 5.31 J/cm Grade Count:21 |
Overview of materials for Polypropylene, Glass Reinforced, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Glass Reinforced, Impact Modified". Each property range of values reported is minimum and.. |
|||
Izod Impact, Unnotched | 4.81 - 10.7 J/cm | 9.00 - 20.0 ft-lb/in | Average value: 6.43 J/cm Grade Count:22 |
Overview of materials for Nylon 6, 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 20% Glass Fiber Filled".Specific grades with glass content between 15% and 24% are included. Ea.. |
|||
Izod Impact, Unnotched | 8.01 - 10.7 J/cm | 15.0 - 20.0 ft-lb/in | ASTM D4812 |
Premix Premi-Glas® 1200-24 Polyester SMC
(discontinued **) Premi-Glas® 1200-24 is a 24% fiberglass-reinforced, thermoset, sheet molding compound designed for Class A Heavy Truck - Bus body panels and Marine cowls parts where smooth, flat, ripple free surfa.. |
|||
Izod Impact, Unnotched | 5.34 - 10.7 J/cm | 10.0 - 20.0 ft-lb/in | Average value: 7.48 J/cm Grade Count:12 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass Filled, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Filled, Impact Modified". Each property range of values reported.. |