Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 1.33 - 1.60 J/cm | 2.50 - 3.00 ft-lb/in | ASTM D256 |
Network Polymers Nylon 6615 L Description: Black Super Tough NylonInformation provided by Network Polymers Inc. |
|||
Izod Impact, Unnotched | 1.33 - 1.60 J/cm @Temperature -40.0 °C |
2.50 - 3.00 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Network Polymers Nylon 6615 L Description: Black Super Tough NylonInformation provided by Network Polymers Inc. |
|||
Izod Impact, Unnotched | 0.900 - 1.60 J/cm | 1.69 - 3.00 ft-lb/in | Notch Status Unknown |
Goodfellow Nickel 70/Copper 30 Alloy Information provided by Goodfellow. |