Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 9.04 J/cm | 16.9 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP PFL38S PA 6 LNP* LUBRICOMP* PFL38S is a compound based on Nylon 6 resin containing 40% Glass Fiber, 15% PTFE. Added features of this material include: Heat Stabilized, Wear Resistant |
|||
Izod Impact, Unnotched | 9.04 J/cm | 16.9 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP RX05496 PA 66 LNP* LUBRICOMP* RX05496 is a compound based on Nylon 66 resin containing 30% Mixed Glass, 15% PTFE, Silicone. Added features of this material include: Wear Resistant. |
|||
Izod Impact, Unnotched | 9.04 J/cm | 16.9 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP RX05496 PA 66 (Asia Pacific) LNP* Lubricomp* RX05496 is a compound based on Nylon 66 resin containing Glass Fiber, PTFE, Silicone. Added features of this material include: Internally Lubricated. |