Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 8.83 J/cm | 16.5 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP DF002 PC LNP THERMOCOMP* DF002 is a compound based on Polycarbonate resin containing 10% Glass Fiber. |
|||
Izod Impact, Unnotched | 8.83 J/cm | 16.5 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP DF002H PC LNP THERMOCOMP* DF002H is a compound based on Polycarbonate resin containing 10% Glass Fiber. Added feature includes: Healthcare. |
|||
Izod Impact, Unnotched | 8.83 J/cm @Thickness 3.17 mm |
16.5 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samyang Trirex® 3025L1 Polycarbonate, Lens Grade TRIREX® polycarbonate resins offer superior transparency, mechanical properties, good dimensional stability and high electrical performance, which allows it to be widely used for electrical, elec.. |
|||
Izod Impact, Unnotched | 8.83 J/cm @Thickness 3.17 mm |
16.5 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samyang Trirex® 3025A Polycarbonate TRIREX® polycarbonate resins offer superior transparency, mechanical properties, good dimensional stability and high electrical performance, which allows it to be widely used for electrical, elec.. |
|||
Izod Impact, Unnotched | 8.83 J/cm | 16.5 ft-lb/in | ASTM D4812 |
LNP Verton™ UF-700-12 Polyphthalamide, Long Glass Fiber Filled
(discontinued **) LNP™ Verton™ UF-700-12 HS EXP is a compound based on Polyphthalamide resin containing Long Glass Fiber. Added features of this material include: Heat Stabilized.Information provided by LNPThis dat.. |