Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 8.81 J/cm @Temperature 23.0 °C |
16.5 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics LNP Stat-kon KS302 Acetal Copoly LNP* Stat-kon* KS302 is a compound based on Acetal Copolymer resin containing Stainless Steel.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Unnotched | 8.81 J/cm | 16.5 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP STAT-KON KS302 Acetal Copoly (Asia Pacific) LNP* Stat-kon* KS302 is a compound based on Acetal Copolymer resin containing Stainless Steel. |
|||
Izod Impact, Unnotched | 8.81 J/cm | 16.5 ft-lb/in | ASTM D4812 |
A. Schulman SCHULADUR® A GF30 30% Glass Fiber Reinforced PBT Information provided by A. Schulman. |
|||
Izod Impact, Unnotched | 8.81 J/cm | 16.5 ft-lb/in | ASTM D4812 |
A. Schulman SCHULADUR® A GF30 30% Glass Fiber Reinforced PBT Information provided by A. Schulman. |
|||
Izod Impact, Unnotched | 8.81 J/cm | 16.5 ft-lb/in | ASTM D4812 |
A. Schulman SCHULADUR® A GF30 30% Glass Fiber Reinforced PBT Information provided by A. Schulman. |
|||
Izod Impact, Unnotched | 8.81 J/cm | 16.5 ft-lb/in | ASTM D4812 |
A. Schulman SCHULADUR® A GF30 30% Glass Fiber Reinforced PBT Information provided by A. Schulman. |
|||
Izod Impact, Unnotched | 8.81 J/cm | 16.5 ft-lb/in | ASTM D4812 |
A. Schulman SCHULADUR® A GF30 30% Glass Fiber Reinforced PBT Information provided by A. Schulman. |
|||
Izod Impact, Unnotched | 8.81 J/cm | 16.5 ft-lb/in | ASTM D4812 |
A. Schulman SCHULADUR® A GF30 30% Glass Fiber Reinforced PBT Information provided by A. Schulman. |