Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 8.55 J/cm | 16.0 ft-lb/in | ASTM D256A |
Total PPH 3825WZ Polypropylene, Injection Molding Grade Easy flow injection molding homopolymerNucleation - FINA 3825WZ is engineered with nucleation to provide fast cycle time and improve contact clarity in thin wall multi-cavity molds.Antistat - FINA 3.. |
|||
Izod Impact, Unnotched | 8.55 J/cm | 16.0 ft-lb/in | ASTM D256A |
Total PPH 3925WZ Polypropylene, Injection Molding Grade Easy flow injection molding homopolymerNucleation - FINA 3925WZ is nucleated to provide fast cycle time and improve contact clarity.Antistat - FINA 3925WZ contains an antistat that will help protect.. |
|||
Izod Impact, Unnotched | 8.55 J/cm | 16.0 ft-lb/in | ASTM D256A |
Total PPH 3825 Polypropylene, Injection Molding Grade Easy flow injection molding homopolymerEasy Flow - FINA 3825 exhibits exceptionally easy flow characteristics.FDA - FINA 3825 complies with all applicable FDA regulations for food contact applicatio.. |