Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 7.58 J/cm | 14.2 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP DFL23 PC (Asia Pacific) LNP* Lubricomp* DFL23 is a compound based on Polycarbonate resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated. |
|||
Izod Impact, Unnotched | 7.58 J/cm | 14.2 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP DFL23 PC LNP* Lubricomp* DFL23 is a compound based on Polycarbonate resin containing 15% Glass Fiber and 10% PTFE. Added features include: Internally Lubricated. |
|||
Izod Impact, Unnotched | 7.58 J/cm | 14.2 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRILOY DF204 PC LNP* LUBRILOY* DF204 is a compound based on Polycarbonate resin containing 20% Glass Fiber, Proprietary Lubricant. Added feature of th is grade is: Wear Resistant. |
|||
Izod Impact, Unnotched | 7.58 J/cm | 14.2 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRILOY RF206 PA 66 (Europe-Africa-Middle East) LNP LUBRILOY* RF206H is a compound based on Nylon 66 resin containing Glass Fiber, Lubricants, Proprietary Lubricant. Added features of this material include: Internally Lubricated. |
|||
Izod Impact, Unnotched | 7.58 J/cm @Temperature 23.0 °C |
14.2 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics LNP Lubriloy RF206H PA 66 LNP LUBRILOY* RF206H is a compound based on Nylon 66 resin containing Glass Fiber, Proprietary Lubricant, Lubricants. Added features of this material include: Internally Lubricated.This data was su.. |
|||
Izod Impact, Unnotched | 7.58 J/cm | 14.2 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRILOY RF206H PA 66 (Asia Pacific) LNP LUBRILOY* RF206H is a compound based on Nylon 66 resin containing Glass Fiber, Lubricants, Proprietary Lubricant. Added features of this material include: Internally Lubricated. |
|||
Izod Impact, Unnotched | 7.58 J/cm | 14.2 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRILOY RF206XXH PA 66 LNP LUBRILOY* RF206H is a compound based on Nylon 66 resin containing 30% Glass Fiber, Proprietary Lubricant. Added features of this material include: Wear Resistant, Healthcare |
|||
Izod Impact, Unnotched | 7.58 J/cm | 14.2 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP EF006 PEI LNP THERMOCOMP* EF006 is a compound based on Polyetherimide resin containing 30% Glass Fiber. |
|||
Izod Impact, Unnotched | 7.58 J/cm | 14.2 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP RX06421S PA 66 (Asia Pacific) LNP* Thermocomp* RX06421S is a compound based on Nylon 66 resin containing Glass Fiber. Added features of this material include: Easy Molding. |