Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 7.47 J/cm | 14.0 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Lexan® FL903 PC Various weight reductions at 0.250"" (6.35 mm). High heat/creep resistance, excellent impact, flexural strength/rigidity. UV-stabilized. |
|||
Izod Impact, Unnotched | 7.47 J/cm | 14.0 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Lexan® FL900 PC (Asia Pacific) Various weight reductions at 0.250"" (6.35 mm). High heat/creep resistance excellent impact, flexural strength/rigidity. UL94 V-1 at .157"" (3.99 mm). |
|||
Izod Impact, Unnotched | 7.47 J/cm | 14.0 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP EL003 PEI LNP LUBRICOMP* EL003 is a compound based on Polyetherimide resin containing 15% PTFE. Added features of this material include: Internally Lubricated. |
|||
Izod Impact, Unnotched | 7.47 J/cm | 14.0 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP EL003 PEI (Europe-Africa-Middle East) LNP LUBRICOMP* EL003 is a compound based on Polyetherimide resin containing PTFE. Added features of this material include: Internally Lubricated. |
|||
Izod Impact, Unnotched | 7.47 J/cm | 14.0 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRILOY DF202P PC LNP LUBRILOY* DF202P is a compound based on Polycarbonate resin containing Glass Fiber, Proprietary Lubricant. Added features of this material include: Wear Resistant, Exceptional Processing. |
|||
Izod Impact, Unnotched | 7.47 J/cm @Temperature 23.0 °C |
14.0 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics Ultem ATX202R PEI+PCE (Europe-Africa-Middle East) 20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Europe-Africa-Middle East regio.. |
|||
Izod Impact, Unnotched | 7.47 J/cm | 14.0 ft-lb/in | ASTM D256 |
Spartech SP-3010 Rigid PVC Specialty Sheet Description: Specialty SheetInformation provided by Spartech. |
|||
Izod Impact, Unnotched | 7.47 J/cm @Thickness 3.17 mm |
14.0 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES Luriblend® PA6 GF40 ML5 HS 12 mm 40% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 40% Filler by WeightAdditive: Heat Stabilized and Molybdenum Disulfide LubricantFeatures: Lubricated and Heat StabilizerAp.. |
|||
Izod Impact, Unnotched | 7.47 J/cm @Thickness 3.17 mm |
14.0 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES Luriblend® PA6/6 GF40 ML2 HS BK 40% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 40% Filler by WeightAdditive: Heat Stabilizer and Molybdenum Disulfide Lubricant(5%)Features: Lubricated and Heat Stabiliz.. |
|||
Izod Impact, Unnotched | 7.47 J/cm @Thickness 3.17 mm |
14.0 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES Luriblend® PA6/6 GF43 ML2 BK 43% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 43% Filler by WeightAdditive: Molybdenum Disulfide Lubricant(2%)Features: Lubricated Appearance: BlackTPCI# 8047101Informa.. |
|||
Izod Impact, Unnotched | 7.47 J/cm | 14.0 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOTUF RF002I PA 66 (Asia Pacific) LNP* THERMOTUF* RF002I is a compound based on Nylon 66 resin containing Glass Fiber. Added features of this material include: High Impact. |
|||
Izod Impact, Unnotched | 7.47 J/cm | 14.0 ft-lb/in | ASTM D4812 |
Asahi Kasei Thermylene® P6-30FG-0699 30% Glass Fiber Reinforced, Heat Stabilized Information provided by Asahi Thermofil |
|||
Izod Impact, Unnotched | 7.47 J/cm | 14.0 ft-lb/in | ASTM D4812 |
A. Schulman SCHULAMID® 66 GF30H 30% Glass Fiber Reinforced, Heat Stabilized Nylon 66 Information provided by A. Schulman. |
|||
Izod Impact, Unnotched | 7.47 J/cm @Thickness 3.17 mm |
14.0 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® PP LGF40 CC HS BK 40% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by WeightAdditive: Heat StabilizerFeatures: Chemically Coupled and Heat StabilizedAppearance: Bla.. |