Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 7.43 J/cm | 13.9 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP DF004P PC (Asia Pacific) LNP* Thermocomp* DF004P is a Polycarbonate base resin containing Glass Fiber. Characteristics of this grade are Exceptional Processing. |