Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 7.08 J/cm | 13.3 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP WF002I PBT LNP* THERMOTUF* WF006I is a compound based on PBT resin containing 10% Glass Fiber. Added feature of this grade is: High Impact. |