Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 6.94 J/cm @Temperature 22.8 °C |
13.0 ft-lb/in @Temperature 73.0 °F |
ASTM D4812 |
Polymer Resources PPX-FR1 Modified-PPO, V-0 Flame Retardant Modified-Polyphenylene Oxide, V-0 Flame Retardant, 190F HDTFeatures: • Bromine Free • Chlorine FreeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-.. |
|||
Izod Impact, Unnotched | 6.94 J/cm | 13.0 ft-lb/in | ASTM D256 |
Polymer Resources TPSF-GP1 PBT, 30% Glass Reinforced Structural Foam Grade Process: Foam MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Foam grades tested with foamed parts with a 10% weight reduction rel.. |
|||
Izod Impact, Unnotched | 6.94 J/cm | 13.0 ft-lb/in | ASTM D4812 |
Solvay Specialty Polymers Supradel® HTS-2420 High Temperature Sulfone Resin
(discontinued **) SUPRADEL HTS-2420 is a 20% glass-fiber reinforced high-temperature, high-performance, amorphous, sulfone polymer. With a glass transition temperature of 245°C and a heat deflection temperature of 2.. |
|||
Izod Impact, Unnotched | 6.94 J/cm @Thickness 3.17 mm |
13.0 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® PP GF40 CC 40% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by WeightFeatures: Chemically CoupledInformation provided by TP Composites, Inc. |
|||
Izod Impact, Unnotched | 6.94 J/cm @Thickness 3.17 mm |
13.0 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES Luriblend® PA6/6 GF33 ML2 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 33% Filler by WeightAdditive: Molybdenum Disulfide Lubricant(2%)Features: LubricatedInformation provided by TP Composites,.. |
|||
Izod Impact, Unnotched | 6.94 J/cm | 13.0 ft-lb/in | ASTM D4812 |
A. Schulman POLYFLAM™ E-14526-31 30% Glass Reinforced Chemically Coupled Polypropylene DescriptionPolyfort® E-14526-31 is a 30% glass reinforced chemically coupled polypropylene black. Information provided by A. Schulman. |
|||
Izod Impact, Unnotched | 6.94 J/cm | 13.0 ft-lb/in | ASTM D256 |
A. Schulman ComAlloy Hiloy® 512 Polycarbonate, Glass Reinforced, UL Data provided by the manufacturer, ComAlloy International Company.20% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Izod Impact, Unnotched | 6.94 J/cm | 13.0 ft-lb/in | ASTM D4812 |
Asahi Kasei Thermylene® P-20FG-1714 20% Glass Fiber Reinforced, Medium Impact Information provided by Asahi Thermofil |
|||
Izod Impact, Unnotched | 6.94 J/cm | 13.0 ft-lb/in | ASTM D4812 |
Asahi Kasei Thermylene® P6-30FG-0632 30% Glass Fiber Reinforced, Heat Stabilized Information provided by Asahi Thermofil |
|||
Izod Impact, Unnotched | 6.94 J/cm | 13.0 ft-lb/in | ASTM D4812 |
A. Schulman POLYFLAM™ E-14526-31 30% Glass Reinforced Chemically Coupled Polypropylene DescriptionPolyfort® E-14526-31 is a 30% glass reinforced chemically coupled polypropylene black. Information provided by A. Schulman. |