Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 5.52 J/cm | 10.3 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP RF0079SZ PA 66 LNP* THERMOCOMP* RF0079SZ is a compound based on Nylon 66 resin containing 35% Glass Fiber. Added features of this material include: Flame Retardant, Heat Stabilized. |
|||
Izod Impact, Unnotched | 5.52 J/cm | 10.3 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP RF0079SZ PA 66 (Asia Pacific) LNP* Thermocomp* RF0079SZ is a compound based on Nylon 66 resin containing Glass Fiber. Added features of this material include: Flame Retardant, Heat Stabilized. |